MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Mitsubishi PPSU 3D Printing Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: PPSU (Polyphenylsulfone) shows even better results in impact resistance and chemical resistance than PEI. It can operate in temperatures up to 180°C. This filament is based on a PPSU grade from Solvay. PPSU is an excellent choice for under-hood automotive applications and medical devices requiring repeated steam sterilization. The hydrolysis resistance is excellent compared to other amorphous thermoplastics. Besides that, it also resists common acids and bases over a broad range of temperatures.

Features:

  • High strength and toughness
  • Excellent chemical and thermal resistance
  • Good hydrolysis resistance
  • Flame retardant
  • Heat resistance up to 220°C
Colors: PPSU is available in the color natural.

Information provided by Mitsubishi Chemical.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.29 g/cc1.29 g/ccASTM D792
Filament Diameter 1750 µm1750 µmTolerance: 50 µm, =95% Roundness
 2850 µm2850 µmTolerance: 100 µm, =95% Roundness
Melt Flow 14 - 20 g/10 min
@Load 5.00 kg,
Temperature 365 °C
14 - 20 g/10 min
@Load 11.0 lb,
Temperature 689 °F
ASTM D1238
Storage Temperature 15.0 - 25.0 °C59.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 77.0 MPa11200 psiISO 527
Tensile Strength, Yield 77.0 MPa11200 psiISO 527
Elongation at Break 60 - 120 %60 - 120 %ISO 527
Elongation at Yield 7.3 %7.3 %ISO 527
Tensile Modulus 2.41 GPa350 ksi(E); ISO 527
Flexural Strength 108 MPa15700 psiISO 178
Flexural Modulus 2.38 GPa345 ksi
Izod Impact, Notched (ISO) 56.2 kJ/m²26.7 ft-lb/in²ISO 180
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Processing Temperature 350 - 390 °C662 - 734 °FPrinting Temperature
Drying Temperature 110 °C230 °F
Dry Time 4.00 hour4.00 hour
 
Descriptive Properties
Bed Temp>140°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMITS9843 / 301068

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.