MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mocom (ALBIS) ALCOM® AWL 109/10 GF20WT1142-12LB ABS, modified with Polycarbonate
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled

Material Notes: Base Polymer: Acrylonitrile/Butadiene/Styrene/Copolymer, modified with Polycarbonate

Filler/Additive System: special filler, 20% glass fibers

Special Features: Highly reflective, opaque, high stiffness

Market Segment: Automotive, Lighting

Application Area: Lighting, light blocking components

Typical Application: Light guides, reflectors

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ISO 1183
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
@Time 86400 sec
0.0020 - 0.0050 in/in
@Time 24.0 hour
ISO 294-4
Melt Flow 8.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
8.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Storage Temperature <= 30.0 °C<= 86.0 °Fdry, protected from light
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 145 MPa21000 psiH358/30; ISO 2039-1
Tensile Strength at Break 65.0 MPa9430 psiISO 527
Elongation at Break 1.0 %1.0 %ISO 527
Tensile Modulus 6.80 GPa986 ksiISO 527
Flexural Strength 100 MPa14500 psiISO 178
Flexural Modulus 6.50 GPa943 ksiISO 178
Charpy Impact Unnotched 1.70 J/cm²8.09 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.550 J/cm²2.62 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FISO 75-1/-2
Vicat Softening Point 112 °C234 °FB50; ISO 306
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 0.10 %
@Thickness 0.500 mm
0.10 %
@Thickness 0.0197 in
ISO 13468
Reflection Coefficient, Visible (0-1) 0.8350.835DIN 5033
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 260 °C464 - 500 °FInjection molding
Mold Temperature 60.0 - 80.0 °C140 - 176 °FInjection molding
Drying Temperature  80.0 - 90.0 °C
@Time 7200 - 14400 sec
176 - 194 °F
@Time 2.00 - 4.00 hour
in a dry air (desiccant) dryer
 80.0 - 90.0 °C
@Time 10800 - 21600 sec
176 - 194 °F
@Time 3.00 - 6.00 hour
in an circulating dryer
 
Descriptive Properties
Base PolymerAcrylonitrile/Butadiene/Styrene/Copolymer, modified with Polycarbonate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PALBIS8448 / 242507

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.