MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultradur® B 4330 G6 HR BK15045 PBT, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Ultradur B 4330 G6 HR BK15045 product is a hydrolysis resistant, pigmented black 30% glass reinforced impact modified injection molding PBT.

Information provided by BASF.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.49 g/cc0.0538 lb/in³ISO 1183
Viscosity Test 106 cm³/g1.06 dl/gISO 1628
Melt Flow 46 g/10 min
@Load 10.0 kg,
Temperature 250 °C
46 g/10 min
@Load 22.0 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 120 MPa17400 psiISO 527
Elongation at Break 3.4 %3.4 %ISO 527
Tensile Modulus 8.50 GPa1230 ksiISO 527
Charpy Impact Unnotched  6.00 J/cm²
@Temperature -30.0 °C
28.6 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 7.40 J/cm²
@Temperature 23.0 °C
35.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 1.40 J/cm²6.66 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 223 °C433 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FISO 75
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 275 °C482 - 527 °F
Mold Temperature 40.0 - 70.0 °C104 - 158 °F
 60.0 - 100 °C140 - 212 °Fupper end of range may be exceeded
Drying Temperature 100 - 120 °C
@Time 14400 sec
212 - 248 °F
@Time 4.00 hour
Moisture Content <= 0.040 %<= 0.040 %
Injection Pressure 3.45 - 10.3 MPa500 - 1500 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASF8907 / 254865

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.