MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Avient Stat-Tech™ LC-20NCF/000 V3 Natural Liquid Crystal Polymer (LCP)
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP)

Material Notes: Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compounds combine the performance of select engineering resins with reinforcing additives such as carbon powder, carbon fiber, nickel-coated carbon fiber and stainless steel fiber for low to high levels of conductivity depending upon application requirements.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.52 g/cc1.52 g/ccASTM D792
Filler Content 20 %20 %Carbon Fiber Reinforcement
Linear Mold Shrinkage, Transverse 0.0070 - 0.010 cm/cm0.0070 - 0.010 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 93.8 MPa13600 psiASTM D638
Elongation at Break 1.0 %1.0 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 15.8 GPa2290 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 145 MPa21000 psiASTM D790
Flexural Modulus 12.2 GPa1770 ksiASTM D790
Izod Impact, Notched 0.270 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
0.506 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 100 - 10000 ohm-cm100 - 10000 ohm-cmASTM D257
Surface Resistance 100 - 10000 ohm100 - 10000 ohmASTM D257
Static Decay 0.0020 sec0.0020 sec(Mil-B-81705C), 12% RH, 500 kV to 50 kV
Shielding Effectiveness 30 - 80 dB
@Frequency 2.0e+7 - 1.80e+10 Hz
30 - 80 dB
@Frequency 2.0e+7 - 1.80e+10 Hz
1/8 thickness
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 260 °C
@Thickness 6.35 mm
500 °F
@Thickness 0.250 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 206 °C
@Thickness 6.35 mm
403 °F
@Thickness 0.250 in
Unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 299 - 316 °C570 - 601 °F
 
Descriptive Properties
FeaturesAntistatic
 Conductive
 Electrically Conductive
 Electromagnetic Shielding (EMI)
 Radio Frequency Shielding (RFI)
 Statically Conductive
FormsPellets
Generic MaterialLCP
Generic NameLiquid Crystal Polymer (LCP)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 South America
RoHS ComplianceRoHS Compliant
UsesAerospace Applications
 Automotive Electronics
 Business Equipment
 Computer Components
 Connectors
 Electrical Housing
 Electrical/Electronic Applications
 Housings

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese VECTRA A950 LCP, Unfilled
RTP Company RTP 3400-3 Liquid Crystal Polymer (LCP), Unfilled
Avient Stat-Tech™ LC-20NCF/000 V3 RD 4020 Liquid Crystal Polymer (LCP)
Avient Stat-Tech™ ST9620-0020 ES Red Liquid Crystal Polymer + PPS (LCP+PPS)
Celanese VECTRAN™ V300P Co-Extrudable Liquid Crystal Polymer (LCP)

PH0POL1066 / 145635

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.