MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Celanese Ateva® 1066BSA Ethylene Vinyl Acetate Copolymer Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: Ateva® 1066BSA resin is suitable for injection molding, blow molding, and extrusion. Additives: Slip / Antiblock

Applications: Flexible Packaging

Information provided by Celanese Corporation.

Key Words: Flexible Packaging
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ASTM D1505; ASTM D1928 Proc A
Vinyl Acetate Content 6.0 %6.0 %AT Plastics PTM-39
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 9.00 MPa1310 psiMethod A (500 mm/min); ASTM D882
Film Tensile Strength at Yield, TD 8.00 MPa1160 psiMethod A (500 mm/min); ASTM D882
Film Elongation at Break, MD 280 %280 %Method A (500 mm/min); ASTM D882
Film Elongation at Break, TD 560 %560 %Method A (500 mm/min); ASTM D882
Secant Modulus, MD 0.115 GPa16.7 ksi1% Secant Modulus; ASTM D882
Secant Modulus, TD 0.145 GPa21.0 ksi1% Secant Modulus; ASTM D882
Dart Drop 6.40 g/micron163 g/milf50; ASTM D1709
Film Tensile Strength at Break, MD 23.0 MPa3340 psiMethod A (500 mm/min); ASTM D882
Film Tensile Strength at Break, TD 22.0 MPa3190 psiMethod A (500 mm/min); ASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 104 °C219 °FDSC; ASTM D3417
Vicat Softening Point 91.0 °C196 °FASTM D1525
Brittleness Temperature -90.0 °C-130 °FASTM D746
 
Optical PropertiesMetricEnglishComments
Haze 26 %26 %ASTM D1003
Gloss 27 %27 %45°; ASTM D2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PBI Performance Products Celazole® PBI U-60 Unfilled Polybenzimidazole Resin
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade
Goodfellow CVD Graphene Film on PET
Diamond, thin film
Bamberger Polymers Bapolene® 4012F Polypropylene, Compounding/Extrusion Grade

PATEVB37 / 25993

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.