MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polypropylene, Film Grade
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.886 - 1.46 g/cc0.0320 - 0.0527 lb/in³Average value: 0.905 g/cc Grade Count:200
Brightness 70.0 - 90.0 %70.0 - 90.0 %Average value: 87.3 % Grade Count:27
Water Vapor Transmission 0.0497 - 1.55 g/m²/day0.00320 - 0.0999 g/100 in²/dayAverage value: 0.968 g/m²/day Grade Count:62
 0.09312 - 18.624 g/m²/day
@Temperature 37.8 - 38.0 °C
0.005997 - 1.1994 g/100 in²/day
@Temperature 100 - 100 °F
Average value: 5.06 g/m²/day Grade Count:184
Oxygen Transmission Rate 0.0931 - 2100 cc/m²/day0.00600 - 135 cc/100 in²/dayAverage value: 375 cc/m²/day Grade Count:74
Thickness 12.0 - 96.5 microns0.472 - 3.80 milAverage value: 31.9 microns Grade Count:361
Linear Mold Shrinkage 0.0100 - 0.0400 cm/cm0.0100 - 0.0400 in/inAverage value: 0.0346 cm/cm Grade Count:102
Linear Mold Shrinkage, Transverse 0.0100 - 0.0180 cm/cm0.0100 - 0.0180 in/inAverage value: 0.0139 cm/cm Grade Count:101
Melt Flow 0.350 - 800 g/10 min0.350 - 800 g/10 minAverage value: 9.10 g/10 min Grade Count:254
Ash 0.00100 - 0.00200 %0.00100 - 0.00200 %Average value: 0.00150 % Grade Count:7
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 55.0 - 11355.0 - 113Average value: 93.3 Grade Count:100
Hardness, Shore D 65.0 - 76.065.0 - 76.0Average value: 71.1 Grade Count:16
Tensile Strength, Ultimate 18.8 - 152 MPa2730 - 22000 psiAverage value: 33.9 MPa Grade Count:32
Film Tensile Strength at Yield, MD 3.00 - 38.6 MPa435 - 5600 psiAverage value: 19.4 MPa Grade Count:22
Film Tensile Strength at Yield, TD 5.90 - 30.4 MPa856 - 4410 psiAverage value: 17.3 MPa Grade Count:19
Tensile Strength, Yield 3.38 - 42.1 MPa490 - 6110 psiAverage value: 32.4 MPa Grade Count:183
Film Elongation at Break, MD 80.0 - 860 %80.0 - 860 %Average value: 217 % Grade Count:308
Film Elongation at Break, TD 5.00 - 1190 %5.00 - 1190 %Average value: 92.9 % Grade Count:289
Elongation at Break 8.00 - 900 %8.00 - 900 %Average value: 375 % Grade Count:46
Elongation at Yield 6.50 - 33.0 %6.50 - 33.0 %Average value: 11.3 % Grade Count:145
Modulus of Elasticity 0.600 - 7.51 GPa87.0 - 1090 ksiAverage value: 2.29 GPa Grade Count:128
Flexural Yield Strength 21.0 - 44.0 MPa3050 - 6380 psiAverage value: 32.1 MPa Grade Count:9
Flexural Modulus 0.220 - 2.28 GPa31.9 - 331 ksiAverage value: 1.36 GPa Grade Count:186
Secant Modulus 0.330 - 0.793 GPa47.9 - 115 ksiAverage value: 0.583 GPa Grade Count:19
Secant Modulus, MD 0.400 - 2.90 GPa58.0 - 420 ksiAverage value: 1.53 GPa Grade Count:31
Secant Modulus, TD 0.500 - 4.83 GPa72.5 - 700 ksiAverage value: 2.53 GPa Grade Count:27
Izod Impact, Notched 0.196 - 5340 J/cm0.367 - 10000 ft-lb/inAverage value: 0.670 J/cm Grade Count:125
 0.180 - 0.340 J/cm
@Temperature -20.0 - 34.0 °C
0.337 - 0.637 ft-lb/in
@Temperature -4.00 - 93.2 °F
Average value: 0.257 J/cm Grade Count:6
Izod Impact, Unnotched 0.342 J/cm - NB0.640 ft-lb/in - NBAverage value: 0.637 J/cm Grade Count:13
 0.392266 - 0.392266 J/cm
@Temperature -10.0 - -10.0 °C
0.734875 - 0.734875 ft-lb/in
@Temperature 14.0 - 14.0 °F
Average value: 0.392 J/cm Grade Count:1
Izod Impact, Notched (ISO) 2.58 - 45.0 kJ/m²1.23 - 21.4 ft-lb/in²Average value: 6.80 kJ/m² Grade Count:26
 2.80 - 7.50 kJ/m²
@Temperature -20.0 - 4.00 °C
1.33 - 3.57 ft-lb/in²
@Temperature -4.00 - 39.2 °F
Average value: 5.43 kJ/m² Grade Count:3
Charpy Impact, Notched 0.340 - 55.0 J/cm²1.62 - 262 ft-lb/in²Average value: 2.80 J/cm² Grade Count:25
 0.140 - 12.0 J/cm²
@Temperature -23.0 - 0.000 °C
0.666 - 57.1 ft-lb/in²
@Temperature -9.40 - 32.0 °F
Average value: 2.40 J/cm² Grade Count:8
Gardner Impact 1.40 - 36.2 J1.03 - 26.7 ft-lbAverage value: 20.6 J Grade Count:6
 28.4722 - 28.4722 J
@Temperature -30.0 - -29.0 °C
21.0000 - 21.0000 ft-lb
@Temperature -22.0 - -20.2 °F
Average value: 32.3 J Grade Count:2
Coefficient of Friction 0.170 - 0.9000.170 - 0.900Average value: 0.352 Grade Count:289
Elmendorf Tear Strength MD 5.00 - 64.0 g5.00 - 64.0 gAverage value: 34.0 g Grade Count:4
Elmendorf Tear Strength TD 70.0 - 300 g70.0 - 300 gAverage value: 150 g Grade Count:4
Elmendorf Tear Strength, MD 0.600 - 1.80 g/micron15.2 - 45.7 g/milAverage value: 1.40 g/micron Grade Count:5
Elmendorf Tear Strength, TD 2.00 - 9.00 g/micron50.8 - 229 g/milAverage value: 4.10 g/micron Grade Count:5
Dart Drop 0.780 - 9.40 g/micron19.8 - 239 g/milAverage value: 2.99 g/micron Grade Count:16
Dart Drop Test 20.0 - 350 g0.0441 - 0.772 lbAverage value: 199 g Grade Count:9
Seal Strength 200 - 410 g/25 mm200 - 410 g/inAverage value: 231 g/25 mm Grade Count:10
 200 - 810 g/25 mm
@Temperature 80.0 - 140 °C
200 - 810 g/in
@Temperature 176 - 284 °F
Average value: 419 g/25 mm Grade Count:65
 200 - 810 g/25 mm
@Pressure 0.00345 - 0.276 MPa
200 - 810 g/in
@Pressure 0.500 - 40.0 psi
Average value: 419 g/25 mm Grade Count:65
Film Tensile Strength at Break, MD 15.0 - 193 MPa2180 - 28000 psiAverage value: 119 MPa Grade Count:391
Film Tensile Strength at Break, TD 7.85 - 310 MPa1140 - 45000 psiAverage value: 228 MPa Grade Count:376
Tangent Modulus 869 - 1620 MPa126000 - 235000 psiAverage value: 1120 MPa Grade Count:3
Heat Seal Strength 518 g/25 mm1.14 lb/inAverage value: 518 g/25 mm Grade Count:48
Heat Seal Strength Initiation Temperature 105 - 130 °C221 - 266 °FAverage value: 113 °C Grade Count:56
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.252.25Average value: 2.25 Grade Count:7
 
Thermal PropertiesMetricEnglishComments
Melting Point 119 - 170 °C246 - 338 °FAverage value: 154 °C Grade Count:78
Deflection Temperature at 0.46 MPa (66 psi) 48.0 - 130 °C118 - 266 °FAverage value: 93.3 °C Grade Count:160
Deflection Temperature at 1.8 MPa (264 psi) 50.0 - 104 °C122 - 219 °FAverage value: 61.7 °C Grade Count:25
Vicat Softening Point 67.0 - 160 °C153 - 320 °FAverage value: 142 °C Grade Count:99
Heat Distortion Temperature 82.0 - 115 °C180 - 239 °FAverage value: 101 °C Grade Count:3
 
Optical PropertiesMetricEnglishComments
Optical Density 1.90 - 3.901.90 - 3.90Average value: 2.49 Grade Count:27
Haze 0.100 - 90.0 %0.100 - 90.0 %Average value: 7.27 % Grade Count:324
Gloss 3.00 - 145 %3.00 - 145 %Average value: 81.0 % Grade Count:366
Transmission, Visible 0.200 - 90.0 %0.200 - 90.0 %Average value: 62.2 % Grade Count:197
 
Processing PropertiesMetricEnglishComments
Processing Temperature 135 - 255 °C275 - 491 °FAverage value: 210 °C Grade Count:5
Melt Temperature 182 - 274 °C360 - 525 °FAverage value: 245 °C Grade Count:34

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene, Extrusion Grade
Overview of materials for Polypropylene, Molded
Overview of materials for Polypropylene, Blow Molding Grade
Overview of materials for Polypropylene with 30% Glass Fiber Filler
Overview of materials for Polypropylene with 10% Glass Fiber Filler

O4707 / 78374

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.