Polyvinyl Chloride Homopolymer having high molecular weight, is white and free-flowing resins produced by suspension polymerization process. The resin can easily blend with variety of additives to achieve desired qualities needed in many applications. The medical grade PVC resin is developed for medicals application which more concerned about health safety. Applications: Medical flexible & sheet, Flexible devices, Nasal tube, Blood tube, Blood bag. Features: Good thermal stability. Low fish eye. Excellent mechanical performance of finished products. Information provided by SCG. |