System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Asahi Kasei Leona™ 14025H Polyamide 66, Heat Stabilized
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, Heat Stabilized
Material Notes:
Applications: Automotive parts, electrical & electronic parts, parts for office furnishings.
Information provided by Asahi Kasei Corp.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.14
g/cc
0.0412
lb/in³
Dry as Molded; ISO 1183
2.50
g/cc
0.0903
lb/in³
Conditioned at 50% RH
Linear Mold Shrinkage, Flow
0.013
-
0.020
cm/cm
0.013
-
0.020
in/in
Asahi Kasei
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell M
55
55
Conditioned at 50% RH; ISO 2039
80
80
Dry as Molded; ISO 2039
Hardness, Rockwell R
108
108
Conditioned; ISO 2039
120
120
Dry as Molded; ISO 2039
Tensile Strength
55.0
MPa
7980
psi
Conditioned at 50% RH; ASTM D638
79.0
MPa
11500
psi
Dry as Molded; ASTM D638
Tensile Strength, Yield
48.0
MPa
6960
psi
Conditioned at 50% RH; ISO 527
82.0
MPa
11900
psi
Dry as Molded; ISO 527
Elongation at Break
>= 50 %
>= 50 %
Conditioned at 50% RH; ISO 527
Elongation at Yield
4.5 %
@Temperature 23.0 °C
4.5 %
@Temperature 73.4 °F
50% RH; ISO 527
25 %
@Temperature 23.0 °C
25 %
@Temperature 73.4 °F
50% RH; ISO 527
Tensile Modulus
1.10
GPa
160
ksi
Conditioned at 50% RH; ISO 527
3.00
GPa
435
ksi
Dry as Molded; ISO 527
Flexural Strength
38.0
MPa
5510
psi
Conditioned at 50% RH
111
MPa
16100
psi
Dry as Molded
Flexural Modulus
0.900
GPa
131
ksi
Conditioned at 50% RH; ISO 178
2.60
GPa
377
ksi
Dry as Molded; ISO 178
Izod Impact, Notched
0.390
J/cm
0.731
ft-lb/in
Dry as Molded; ASTM D256
1.96
J/cm
3.67
ft-lb/in
Conditioned at 50% RH; ASTM D256
Charpy Impact Unnotched
NB
NB
Conditioned at 50% RH; ISO 179
NB
NB
Dry as Molded; ISO 179
Charpy Impact, Notched
0.600
J/cm²
2.86
ft-lb/in²
Dry as Molded; ISO 179
1.60
J/cm²
7.61
ft-lb/in²
Conditioned at 50% RH; ISO 179
Taber Abrasion, mg/1000 Cycles
7.0
7.0
Conditioned at 50% RH; ASTM D1044
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+14
ohm-cm
1.00e+14
ohm-cm
Dry as Molded; IEC 60093
Surface Resistance
1.00e+13
ohm
1.00e+13
ohm
Dry as Molded; IEC 60093
Dielectric Strength
20.0
kV/mm
508
kV/in
Dry as Molded; IEC 60243
Comparative Tracking Index
525
V
@Thickness 3.00 mm
525
V
@Thickness 0.118 in
Dry as Molded; IEC 60112
Thermal Properties
Metric
English
Comments
CTE, linear
80.0
µm/m-°C
44.4
µin/in-°F
Dry as Molded; ASTMD 696
Specific Heat Capacity
1.67
J/g-°C
0.399
BTU/lb-°F
Dry as Molded
Thermal Conductivity
0.200
W/m-K
1.39
BTU-in/hr-ft²-°F
Dry as Molded
Deflection Temperature at 0.46 MPa (66 psi)
162
°C
324
°F
Dry as Molded; ISO 75
Deflection Temperature at 1.8 MPa (264 psi)
62.0
°C
144
°F
Dry as Molded; ISO 75
Flammability, UL94
V-2
@Thickness 0.750 mm
V-2
@Thickness 0.0295 in
Dry as Molded
Oxygen Index
26 %
26 %
Dry as Molded; ASTM D2863
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PASAHI8123 / 221150
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.