MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Universal Wire Works A286 (AMS 5804) Filler Metal
Categories: Metal; Ferrous Metal; Stainless Steel; Superalloy; Iron Base

Material Notes: Primarily used to inert-gas-arc weld base metals of similar composition requiring joints with strength, corrosion and heat resistance comparable to those of the base metal.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesMetricEnglishComments
Boron, B 0.0060 %0.0060 %
Chromium, Cr 15 %15 %
Iron, Fe >= 55.7 %>= 55.7 %As Remainder
Molybdenum, Mo 1.3 %1.3 %
Nickel, Ni 25.5 %25.5 %
Titanium, Ti 2.2 %2.2 %
Vanadium, V 0.30 %0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A286 IRON BASED 15Cr-26Ni-1.3Mo-2.1Ti-0.3V SUPERALLOY FORGINGS FOR GAS TURBINE DISCS
ATI Allegheny Ludlum Altemp® A286 Iron-Base Superalloy, UNS S66286
660 Stainless Steel (A286) cold drawn wire diameter of 5.61 mm, aged at 425°C (800°F)
660 Stainless Steel (A286) short time tensile test
660 Stainless Steel (A286) cold drawn wire diameter of 5.61 mm

NUWW314 / 19743

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.