MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Mitsui TPX® MX002 Methylpentene Copolymer
Categories: Polymer; Thermoplastic; Polymethylpentene (PMP)

Material Notes: TPX® is a 4-methylpentene-1 based polyolefin. TPX is used in a wide variety of applications, including: medical equipment, laboratory ware, small appliances, ovenware, baking cartons, release paper, wire and cable coating, and a number of industrial uses. TPX is manufactured and marketed solely by Mitsui Chemicals, Inc.

Applications:

  • Injection Molded Items:
    • Blood test cells
    • Medical instruments
    • Laboratory ware
    • Coffee maker parts
    • Cosmetic containers
  • Extrusion Molded Items:
    • Sight glass (pipes, sheets)
    • Baking cartons (food containers)
    • Release paper
    • Wire and cable coating
    • Films

Molding Method:

  • Injection
  • Extrusion
  • Blow

Information provided by Mitsui.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.835 g/cc0.0302 lb/in³ASTM D1505
Water Absorption 0.010 %0.010 %24 hours; ASTM D570
Linear Mold Shrinkage 0.016 cm/cm0.016 in/inMPC method, MD
Linear Mold Shrinkage, Transverse 0.016 cm/cm0.016 in/inMPC method
Melt Flow 22 g/10 min
@Load 5.00 kg,
Temperature 260 °C
22 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 3535ASTM D785
Tensile Strength at Break 15.7 MPa2280 psi5mm/min; ASTM D638
Tensile Strength, Yield 14.7 MPa2130 psi5mm/min; ASTM D638
Elongation at Break 120 %120 %MPC method, 5mm/min
Modulus of Elasticity 0.490 GPa71.1 ksiTangent; ASTM D790
Flexural Strength 19.6 MPa2840 psi2mm/min; ASTM D790
Flexural Stiffness 386 MPa56000 psiOlsen Stiffness; ASTM D747
Izod Impact, Unnotched (ISO) 48.3 kJ/m²
@Thickness 2.00 mm,
Temperature 20.0 °C
23.0 ft-lb/in²
@Thickness 0.0787 in,
Temperature 68.0 °F
ASTM D256
Charpy Impact, Notched 0.420 J/cm²
@Thickness 2.00 mm,
Temperature 20.0 °C
2.00 ft-lb/in²
@Thickness 0.0787 in,
Temperature 68.0 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.12
@Frequency 100 - 1.00e+6 Hz
2.12
@Frequency 100 - 1.00e+6 Hz
ASTM D150
Dielectric Strength 63.0 kV/mm1600 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 117 µm/m-°C
@Temperature 20.0 °C
65.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Specific Heat Capacity 1.97 J/g-°C0.471 BTU/lb-°FASTM C351
Thermal Conductivity 0.167 W/m-K1.16 BTU-in/hr-ft²-°FBS 874A
Melting Point 235 °C455 °FMPC Method
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C176 °FASTM D648
Vicat Softening Point 145 °C293 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4631.463n20 D; ASTM D542
Haze 2.0 %2.0 %ASTM D1746
Transmission, Visible 90 %90 %Mfr. indicates clear but does not quantify
 
Descriptive Properties
AppearanceColorless transparent
Rate of Burning2.54 cm/minASTM D635

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsui TPX® MX004 Methylpentene Copolymer
Mitsui TPX® RT18 Methylpentene Copolymer, Transparent Grade
Mitsui TPX® DX820 Methylpentene Copolymer
Mitsui TPX® RT18 XB Methylpentene Copolymer
Westlake Plastics TPX® Polymethylpentene

PMIT049 / 53230

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.