MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PBI Performance Products Celazole® PBI U-60 ESD E5 Polybenzimidazole Resin, 15% Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polybenzimidazole (PBI)

Material Notes: Celazole® U-60 ESD is an electro-static dissipative (ESD) variant of U-60 available as a stock shape or part. U-60 ESD incorporates carbon fiber to increase the conductivity of the finished part and is often used where static discharge is a concern.

Information provided by PBI Performance Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.38 g/cc1.38 g/cc
Filler Content 15.0 %15.0 %Carbon Fiber
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 96.096.0ASTM D2240
Tensile Strength at Break 200 MPa29000 psiASTM D638
Elongation at Break 2.50 %2.50 %ASTM D638
Tensile Modulus 9.00 GPa1310 ksiASTM D638
Flexural Yield Strength 260 MPa37700 psiASTM D790
Flexural Modulus 9.70 GPa1410 ksiASTM D790
Compressive Strength 430 MPa62400 psiASTM D695
Izod Impact, Notched 0.294 J/cm
@Thickness 3.17 mm
0.550 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 10000 - 1.00e+6 ohm10000 - 1.00e+6 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.0 µm/m-°C
@Temperature 25.0 - 150 °C
8.89 µin/in-°F
@Temperature 77.0 - 302 °F
ASTM D695
Glass Transition Temp, Tg 427 °C801 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPBIP001b / 326942

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.