MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arkema Pebax® 7033 SP 01 Polyether Block Amide (PEBA)
Categories: Polymer; Thermoplastic; Polyether Block Amide (PEBA)

Material Notes: Polyether block amide PEBAX® 7033 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ISO 1183
 1.01 g/cc0.0365 lb/in³Cond.; ISO 1183
 0.830 g/cc
@Temperature 260 °C
0.0300 lb/in³
@Temperature 500 °F
Melt
Water Absorption 1.1 %1.1 %Dry; Sim. to ISO 62
Moisture Absorption 0.700 %0.700 %Dry; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.012 cm/cm0.012 in/inDry; ISO 294-4, 2577
 0.015 cm/cm0.015 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 61
@Time 15.0 sec
61
@Time 0.00417 hour
Dry; ISO 7619-1
Tensile Strength at Break 54.0 MPa7830 psiDry; ISO 527-1/-2
Tensile Strength, Yield 22.0 MPa3190 psiCond.; ISO 527-1/-2
 23.0 MPa3340 psiDry; ISO 527-1/-2
Tensile Stress at Strain 22.0 MPa
@Strain 10 %
3190 psi
@Strain 10 %
Dry; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %Dry; ISO 527-1/-2
 >= 50 %>= 50 %Cond.; ISO 527-1/-2
 >= 300 %>= 300 %Dry; ISO 527-1/-2
Elongation at Yield 20 %20 %Cond.; ISO 527-1/-2
 22 %22 %Dry; ISO 527-1/-2
Tensile Modulus 0.390 GPa56.6 ksiCond.; ISO 527-1/-2
 0.414 GPa60.0 ksiDry; ISO 527-1/-2
100% Modulus 21.0 MPa
@Strain 100 %
3050 psi
@Strain 100 %
Dry; ISO 527-1/-2
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Dry; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Cond.; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Cond.; ISO 179/1eU
Charpy Impact, Notched  2.00 J/cm²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
Cond.; ISO 179/1eA
 12.0 J/cm²
@Temperature 23.0 °C
57.1 ft-lb/in²
@Temperature 73.4 °F
Cond.; ISO 179/1eA
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry; ISO 179/1eA
Tear Strength 149 kN/m850 pliDry; ISO 34-1
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 4.00e+13 ohm4.00e+13 ohmCond.; IEC 60093
Comparative Tracking Index 600 V600 VCond.; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 160 µm/m-°C88.9 µin/in-°FDry; ISO 11359-1/-2
Specific Heat Capacity 2.70 J/g-°C0.645 BTU/lb-°FMelt
Thermal Conductivity 0.200 W/m-K
@Temperature 260 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 500 °F
Melt
Melting Point 172 °C342 °F10°C/min; Dry; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °C210 °FDry; ISO 75-1/-2
Vicat Softening Point 164 °C327 °F50°C/h 50N; Dry; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °FInjection Molding; ISO 294
Mold Temperature 60.0 °C140 °FInjection Molding; ISO 10724
Injection Velocity 200 mm/sec7.87 in/secInjection Molding; ISO 294
Hold Pressure 30.0 MPa4350 psiInjection Molding; ISO 294
 
Descriptive Properties
Form as DeliveredPellets
Heat StabilizedYes
Light StabilizedYes
Moisture SensitiveYes
Processing MethodsCasting
 Film Extrusion
 Injection Molding
 Other Extrusion
 Profile Extrusion
 Thermoforming
 Transfer Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Pebax® 7233 SA 01 MED Polyether Block Amide (PEBA)
Arkema Pebax® 6333 SP 01 Polyether Block Amide (PEBA)
Arkema Pebax® 7033 SA 01 MED Polyether Block Amide (PEBA)
Arkema Pebax® 7233 SP 01 TPA
Arkema Pebax® 5533 SP 01 Polyether Block Amide (PEBA)

PARKG722 / 142517

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.