MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman BMC T10(14) General Purpose Molding Compound
Categories: Polymer; Thermoset; Polyester, TS; Polyester (Thermoset) - Rigid

Material Notes: BMC T10(14) is a general purpose, low shrink molding compound. Due to the excellent flow and controlled reactivity, BMC T10(14) is well suited for injection, transfer or compression molding of intricate parts. Typical applications are circuit breakers, insulators, bobbins and electrical connectors.

Information provided by Bulk Molding Compounds, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.87 - 2.07 g/cc0.0676 - 0.0748 lb/in³Molded
Linear Mold Shrinkage 0.0017 - 0.0022 cm/cm0.0017 - 0.0022 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 30 - 4030 - 40
Tensile Strength 57.2 - 71.0 MPa8300 - 10300 psi
Flexural Strength 116 - 143 MPa16800 - 20800 psi
Flexural Modulus 8.96 - 10.3 GPa1300 - 1500 ksi
Compressive Strength 162 - 190 MPa23500 - 27500 psi
Izod Impact, Notched 2.78 - 3.84 J/cm5.20 - 7.20 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 13.8 - 15.8 kV/mm351 - 401 kV/inshort time
Arc Resistance >= 181 sec>= 181 sec
Comparative Tracking Index >= 500 V>= 500 V
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C>= 500 °F
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Processing Temperature 138 - 166 °C280 - 330 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman BMC T12-15526 General Purpose Molding Compound
A. Schulman BMC 400 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade

PBMC928 / 123392

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.