MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Celanese Zytel® HTN (PA6T/66) HTNFR52G35NHF BK337 PA(6T/66)-GF35FR(40)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 40% Glass Fiber Reinforced

Material Notes: 35% Glass Reinforced, Flame Retardant, Non-Halogenated, PPA, High Performance Polyamide with Improved Flow

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.49 g/cc0.0538 lb/in³DAM; ISO 1183
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/inDAM; ISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 135 MPa19600 psiDAM; ISO 527-1/-2
Elongation at Break 1.4 %1.4 %DAM; ISO 527-1/-2
Tensile Modulus 12.8 GPa1860 ksiDAM; ISO 527-1/-2
Flexural Strength 200 MPa29000 psiDAM; ISO 178
Flexural Modulus 11.2 GPa1620 ksiDAM; ISO 178
Poissons Ratio 0.330.33DAM
Charpy Impact, Notched  0.800 J/cm²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 0.800 J/cm²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.9
@Frequency 1e+6 Hz
3.9
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 4.3
@Frequency 100 Hz
4.3
@Frequency 100 Hz
DAM; IEC 62631-2-1
Dielectric Strength 31.0 kV/mm787 kV/inDAM; IEC 60243-1
Dissipation Factor  0.0050
@Frequency 100 Hz
0.0050
@Frequency 100 Hz
DAM; IEC 62631-2-1
 0.011
@Frequency 1e+6 Hz
0.011
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
Comparative Tracking Index 600 V600 VDAM; IEC 60112
 >= 600 V
@Thickness 3.00 mm
>= 600 V
@Thickness 0.118 in
PLC 0; DAM; UL 746A
 
Thermal PropertiesMetricEnglishComments
Melting Point 310 °C590 °Ffirst heat; DAM; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 283 °C541 °FDAM; ISO 75-1/-2
Glass Transition Temp, Tg 45.0 °C113 °F10°C/min; 50% RH; ISO 11357-1/-2
 90.0 °C194 °F10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94  V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
DAM; IEC 60695-11-10
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
DAM; IEC 60695-11-10
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
<= 3.15 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
Oxygen Index 33 %33 %DAM; ISO 4589-1/-2
Glow Wire Ignition Temperature  775 °C
@Thickness 0.750 mm
1430 °F
@Thickness 0.0295 in
DAM; IEC 60695-2-13
 775 °C
@Thickness 1.50 mm
1430 °F
@Thickness 0.0591 in
DAM; IEC 60695-2-13
 850 °C
@Thickness 3.00 mm
1560 °F
@Thickness 0.118 in
DAM; IEC 60695-2-13
 
Processing PropertiesMetricEnglishComments
Melt Temperature 320 - 325 °C608 - 617 °FRange, Injection
Mold Temperature 90.0 - 130 °C194 - 266 °FInjection
Drying Temperature 100 °C212 °FInjection
Dry Time 6.00 - 8.00 hour6.00 - 8.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.10 %<= 0.10 %Injection
 
Descriptive Properties
AdditivesFlame retardant
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
ISO designationISO 16396-PA6T/66,GF35 FR(40),M1CF1G,S10-120
Part Marking Code>PA(6T/66)-GF35FR(40)<ISO 11469
 >PPA-GF35FR<SAE J1344
PolymerPA6T/66-GF35 FR(40)
Resin IdentificationPA(6T/66)-GF35FR(40)ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSX5465h / 254535

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.