MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Akulon® F132-E1 PA6, Medium/High Viscosity, Nucleated, Lubricated, Film Extrusion
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Film Grade; Nylon 6, Nucleated

Material Notes: Medium/High Viscosity, Nucleated, Lubricated, Film Extrusion

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Water Vapor Transmission 35.0 g/m²/day2.25 g/100 in²/dayDIS 15106-1/-3
Oxygen Transmission 1.00 cc-mm/m²-24hr-atm2.54 cc-mil/100 in²-24hr-atm0% RH; DIS 15105-1/-2
 1.55 cc-mm/m²-24hr-atm3.94 cc-mil/100 in²-24hr-atm85% RH; DIS 15105-1/-2
Viscosity 1120 cP
@Temperature 260 °C
1120 cP
@Temperature 500 °F
Melt; DSM Method
 50 cP
@Shear Rate 10000 1/s,
Temperature 280 °C
50 cP
@Shear Rate 10000 1/s,
Temperature 536 °F
 50 cP
@Shear Rate 10000 1/s,
Temperature 260 °C
50 cP
@Shear Rate 10000 1/s,
Temperature 500 °F
 50 cP
@Shear Rate 10000 1/s,
Temperature 240 °C
50 cP
@Shear Rate 10000 1/s,
Temperature 464 °F
 500 cP
@Shear Rate 100 1/s,
Temperature 280 °C
500 cP
@Shear Rate 100 1/s,
Temperature 536 °F
 600 cP
@Shear Rate 0.1 1/s,
Temperature 280 °C
600 cP
@Shear Rate 0.1 1/s,
Temperature 536 °F
 700 cP
@Shear Rate 100 1/s,
Temperature 260 °C
700 cP
@Shear Rate 100 1/s,
Temperature 500 °F
 1000 cP
@Shear Rate 100 1/s,
Temperature 240 °C
1000 cP
@Shear Rate 100 1/s,
Temperature 464 °F
 1000 cP
@Shear Rate 0.1 1/s,
Temperature 260 °C
1000 cP
@Shear Rate 0.1 1/s,
Temperature 500 °F
 2500 cP
@Shear Rate 0.1 1/s,
Temperature 240 °C
2500 cP
@Shear Rate 0.1 1/s,
Temperature 464 °F
Viscosity Number 210 cm³/g2.10 dl/gISO 307, 1157, 1628
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 34.0 MPa4930 psiISO 527-3
Film Elongation at Break, MD 350 %350 %ISO 527-3
Modulus of Elasticity 0.465 GPa67.4 ksi50 mm/min; DSM Method
Coefficient of Friction, Dynamic 0.800.80ISO 8295
Coefficient of Friction, Static 1.41.4ISO 8295
Tear Strength Test 3232Trouser Tear resistance, parallel; ISO 6383-1
Film Tensile Strength at Break, MD 96.0 MPa13900 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C50.0 µin/in-°FISO 11359-1/-2
Specific Heat Capacity 1.55 J/g-°C0.370 BTU/lb-°F
 2.25 J/g-°C
@Temperature 20.0 - 150 °C
0.538 BTU/lb-°F
@Temperature 68.0 - 302 °F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 85 %85 %DSM Method
 
Processing PropertiesMetricEnglishComments
Processing Temperature 270 °C518 °FExtruder
Die Temperature 270 °C518 °F
Roll Temperature 110 °C230 °FChill
 
Descriptive Properties
Puncture resistance1230 J/mDSM Method
RSV formic acid3.2[1g/100ml], DSM Method
Type of extrusionCast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Akulon® F130-E1 PA6, Medium Viscosity, Nucleated, Lubricated, Film Extrusion
Envalior Akulon® F223-D PA6, Conditioned, Low/Medium Viscosity
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Conditioned)
Envalior Akulon® F132-C1 PA6
Envalior Akulon® F136-E1 PA6, Very High Viscosity, Nucleated, Lubricated, Film Extrusion

PDSM8007 / 184708

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.