  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

AISI Type A6 Tool Steel, austenitized 830-870°C (1525-1600°F)
Categories: Metal; Ferrous Metal; Tool Steel; Air-Hardening Steel; Cold Work Steel

Material Notes: High hardenability, high dimensional stability in heat treatment. Good wear resistance, fatigue life, and toughness.

Key Words: UNS T30106, ASTM A681, FED QQ-T-570
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.03 g/cc0.290 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 724724Converted from Rockwell C hardness.
Hardness, Rockwell C 6060
Hardness, Vickers 703703
Tensile Strength, Ultimate 2380 MPa345000 psi
Tensile Strength, Yield 2100 MPa305000 psi
Elongation at Break 1.0 %1.0 %in 50 mm
Modulus of Elasticity 203 GPa29400 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.8 µm/m-°C
@Temperature 20.0 - 100 °C
6.56 µin/in-°F
@Temperature 68.0 - 212 °F
 13.2 µm/m-°C
@Temperature 0.000 - 300 °C
7.33 µin/in-°F
@Temperature 32.0 - 572 °F
 14.1 µm/m-°C
@Temperature 0.000 - 500 °C
7.83 µin/in-°F
@Temperature 32.0 - 932 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 150 - 425 °C302 - 797 °FTempering Temperature
 830 - 870 °C1530 - 1600 °FHardening Temperature
Annealing Temperature 730 - 745 °C1350 - 1370 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.65 - 0.75 %0.65 - 0.75 %
Chromium, Cr 0.90 - 1.2 %0.90 - 1.2 %
Iron, Fe 93.8 - 95.8 %93.8 - 95.8 %As Balance
Manganese, Mn 1.8 - 2.5 %1.8 - 2.5 %
Molybdenum, Mo 0.90 - 1.2 %0.90 - 1.2 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si <= 0.50 %<= 0.50 %
Sulfur, S <= 0.030 %<= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type A6 Tool Steel
AISI Type A2 Tool Steel
AISI Type A3 Tool Steel
AISI Type A5 Tool Steel
AISI Type A4 Tool Steel

MSTA6 / 14249

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.