MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Grade 705 Zirconium (Zr-2.5Nb)
Categories: Metal; Nonferrous Metal; Zirconium Alloy

Material Notes: Characteristics:
  • Higher strength than Zircaloys
  • High corrosion resistance to super-heated water, yet lower than the Zircaloys
  • Forms a stable, dense, self-healing oxide layer
  • Highly anisotropic

Applications: Pressure tubes in heavy water reactors

Machining Parameters: Use slow speeds, heavy feeds and flood cooling with a water-soluble oil lubricant.

Key Words: UNS R60705, Zircadyne® 705
Vendors: Eagle Alloys Corporation is a leading supplier of quality metals and alloys. Our staff prides itself on working fast, efficiently and courteously to get you the information you need. Call (800) 237-9012 or visit www.EagleAlloys.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 6.44 g/cc0.233 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate >= 552 MPa>= 80100 psi
 260 MPa
@Temperature 400 °C
37700 psi
@Temperature 752 °F
 300 MPa
@Temperature 300 °C
43500 psi
@Temperature 572 °F
 370 MPa
@Temperature 200 °C
53700 psi
@Temperature 392 °F
 480 MPa
@Temperature 100 °C
69600 psi
@Temperature 212 °F
 600 MPa
@Temperature 20.0 °C
87000 psi
@Temperature 68.0 °F
Tensile Strength, Yield  150 MPa
@Temperature 400 °C
21800 psi
@Temperature 752 °F
 190 MPa
@Temperature 300 °C
27600 psi
@Temperature 572 °F
 270 MPa
@Temperature 200 °C
39200 psi
@Temperature 392 °F
 370 MPa
@Temperature 100 °C
53700 psi
@Temperature 212 °F
 500 MPa
@Temperature 20.0 °C
72500 psi
@Temperature 68.0 °F
 >= 379 MPa
@Strain 0.2 %
>= 55000 psi
@Strain 0.2 %
Elongation at Break 16 %16 %in 50 mm
 20 %
@Temperature 20.0 °C
20 %
@Temperature 68.0 °F
 27 %
@Temperature 400 °C
27 %
@Temperature 752 °F
 30 %
@Temperature 300 °C
30 %
@Temperature 572 °F
 32 %
@Temperature 100 °C
32 %
@Temperature 212 °F
 34 %
@Temperature 200 °C
34 %
@Temperature 392 °F
Modulus of Elasticity 97.9 GPa14200 ksi
Poissons Ratio 0.330.33
Shear Modulus 34.5 GPa5000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000550 ohm-cm0.0000550 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.30 µm/m-°C
@Temperature 25.0 °C
3.50 µin/in-°F
@Temperature 77.0 °F
Specific Heat Capacity 0.285 J/g-°C0.0681 BTU/lb-°F
Thermal Conductivity 17.1 W/m-K119 BTU-in/hr-ft²-°F
Melting Point 1840 °C3340 °F
Boiling Point 4380 °C7920 °F
 
Component Elements PropertiesMetricEnglishComments
Fe + Cr 0.20 %0.20 %
Hafnium, Hf <= 4.5 %<= 4.5 %
Niobium, Nb (Columbium, Cb) 2.5 %2.5 %
Oxygen, O 0.18 %0.18 %
Zirconium, Zr >= 95.5 %>= 95.5 %includes Hf
 
Descriptive Properties
Alpha plus Beta Phase Crystal Structurehcp + bcc954°C
Beta Phase Crystal Structurebcc> 854°C

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zr-2.5Nb Zirconium Alloy, Nuclear Grade
Grade 702 Zirconium, Commercially Pure
Grade 706 Zirconium (Zr-2.5Nb)
Zircaloy-4 Zirconium Alloy
Reactor Grade Zirconium

MZRI20 / 14572

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.