MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Evonik VESTOPLAST® 828 Amorphous Polyalphaolefin
Categories: Polymer; Thermoplastic; Polyalphaolefin

Material Notes: VESTOPLAST 828 is a amorphous polyalphaolefin and propene-rich. Generally used as hot melt adhesives for the furniture sector and structural bonds.

Key Words: APAO
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.870 g/cc
@Temperature 23.0 °C
0.0314 lb/in³
@Temperature 73.4 °F
Viscosity 18000 - 32000 cP
@Temperature 190 °C
18000 - 32000 cP
@Temperature 374 °F
melt, rotational viscometer; DIN 53 019
Molecular Weight 13200 g/mol13200 g/molMn; GPC
 61000 g/mol61000 g/molMw; GPC
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5555DIN 53 505
Tensile Strength at Break 1.00 MPa145 psiDIN EN ISO 527-3
Elongation at Break 550 %550 %DIN EN ISO 527-3
Shear Modulus 0.00400 GPa
@Temperature 23.0 °C
0.580 ksi
@Temperature 73.4 °F
DIN EN ISO 6721-2
Penetration 19 - 25
@Thickness 0.100 mm
19 - 25
@Thickness 0.00394 in
needle 100/25/5; DIN 52 010
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 95.0 - 100 °C203 - 212 °Funder load 5 °C/h, weight 450g; Degussa Method
Glass Transition Temp, Tg -35.0 °C-31.0 °FDSC
Ring & Ball Softening Point 157 - 165 °C315 - 329 °FDIN 52 011
 
Descriptive Properties
Open Time (sec)70Degussa Method
Setting Time (sec)1Degussa Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik VESTOPLAST® 703 Amorphous Polyalphaolefin
Evonik VESTOPLAST® 888 Amorphous Polyalphaolefin
Evonik VESTOPLAST® 608 Amorphous Polyalphaolefin
Evonik VESTOPLAST® 704 Amorphous Polyalphaolefin
Evonik VESTOPLAST® 792 Amorphous Polyalphaolefin

PHUMB423 / 81425

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.