Celanese Celstran® PP-GF50-02- Natural PP, 50% Glass Reinforced
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene with 50% Glass Fiber Filler
Material Notes:
50% long strand glass fiber chemically coupled polypropylene, Natural
Information provided by Celanese
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.33
g/cc
1.33
g/cc
ASTM D792
Density
1.33
g/cc
0.0480
lb/in³
ISO 1183
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
121
MPa
17500
psi
ASTM D638
148
MPa
21500
psi
5mm/min; ISO 527-2/1A
Elongation at Break
1.4 %
1.4 %
ASTM D638
1.9 %
1.9 %
5mm/min; ISO 527-2/1A
Tensile Modulus
11.0
GPa
1600
ksi
ASTM D638
11.6
GPa
1680
ksi
50mm/min; ISO 527-2/1A
Flexural Strength
193
MPa
28000
psi
ASTM D790
252
MPa
36500
psi
ISO 178
Flexural Modulus
9.58
GPa
1390
ksi
ASTM D790
12.0
GPa
1740
ksi
ISO 178
Izod Impact, Notched
2.99
J/cm
5.60
ft-lb/in
ASTM D256
Charpy Impact, Notched
4.40
J/cm²
20.9
ft-lb/in²
ISO 179/1eA
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
154
°C
310
°F
ASTM D648
Processing Properties
Metric
English
Comments
Processing Temperature
40.0
-
70.0
°C
104
-
158
°F
cavity
Feed Temperature
20.0
-
50.0
°C
68.0
-
122
°F
Zone 1
220
-
230
°C
428
-
446
°F
Zone 2
220
-
230
°C
428
-
446
°F
Zone 3
230
-
250
°C
446
-
482
°F
Zone 4
230
-
250
°C
446
-
482
°F
Die Temperature
230
-
250
°C
446
-
482
°F
Melt Temperature
230
-
250
°C
446
-
482
°F
Drying Temperature
90.0
-
100
°C
194
-
212
°F
Dry Time
2.00
hour
2.00
hour
Moisture Content
<= 0.20 %
<= 0.20 %
Descriptive Properties
Injection molding
Yes
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Celanese Celstran® PP-GF50-02-Black PP, 50% Glass Reinforced
Techmer ES HiFill® PP GF50 CC HF BK 50% Glass Filled
Asahi Kasei Thermylene® P6-50FG-0100 PP-GF50
Celanese Celstran® PP-GF50-03-Black PP, 50% Glass Reinforced
Techmer ES HiFill® PP GF15 CC 15% Glass Filled
PHCQ233 / 178688
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.