MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Magnesium Elektron Elektron® 43 Magnesium Alloy  (Unverified Data**)
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: Elektron 43 is a light, high strength wrought magnesium alloy for use at temperatures up to 250°C. Designs in Elektron 43 can be 20% to 30% lighter than a corresponding aluminium design. Elektron 43 is available as rolled plate, forging feedstock and extruded bar, section & profile. Elektron 43 is an optimized wrought evolution of the original casting alloy, Elektron WE43. The properties of Elektron 43 mean it is well suited for use as feedstock material from which to machine high performance components, especially those associated with elevated temperature performance. Elektron 43 has undergone extensive flammability testing by the Federal Aviation Administration (FAA). The FAA have shown that the use of Elektron 43 in aircraft seat frames does not reduce the level of safety of the aircraft when compared to heavier aluminium seat components.

Information provided by Magnesium Elektron

Vendors:
Available Properties
  • Specific Gravity
  • Hardness, Brinell
  • Tensile Strength at Break, Extruded Bar, Transverse
  • Tensile Strength at Break, Extruded Bar, Longitudinal
  • Tensile Strength at Break
  • Tensile Strength at Break
  • Tensile Strength, Ultimate, Longitudinal-Specification min
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Stress, 0.2% Proof, Extruded Bar, Transverse
  • Tensile Stress, 0.2% Proof, Longitudinal-Specification min
  • Tensile Stress, 0.2% Proof, Extruded Bar, Longitudinal
  • Tensile Stress, 0.2% Proof
  • Tensile Stress, 0.2% Proof
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Elongation at Break, Longitudinal-Specification min
  • Elongation at Break, Extruded Bar, Transverse
  • Elongation at Break, Extruded Bar, Longitudinal
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Modulus of Elasticity
  • Poissons Ratio
  • Electrical Resistivity
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Magnesium, Mg
  • Rare Earths
  • Yttrium, Y
  • Zirconium, Zr
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.