Features: Good Chemical Resistance; Good Electrical Properties; Good Strength
Additional Properties: Heat Deflection Temperature - ASTM D648 265 °C; Insulation Resistance - (90°C): 1.00E+13 ohm; Mold Shrinkage - 0.20 %; Mold Shrinkage - 0.40 %; Temperature Index - UL 746B 220 to 240 °C
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlastic