MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Refractory Metals
Plansee MoOx Molybdenum Oxide Sputtering Target
Categories: Ceramic; Oxide

Material Notes: Used for the manufacture of highly absorbent functional layers.

Molybdenum oxide layers, with their low level of optical reflection, have a wide range of applications in modern flat screens. Uses include reliable separation of subpixels, an elegant way of covering conductor strips, or the prevention of unwanted reflections from the ambient light. PLANSEE supplies different chemical compositions of MoOx in the form of planar targets for producing these layers.

Property data for Mo-31.5%O by weight.

Information provided by PLANSEE.

Vendors:
Available Properties
  • Density
  • Electrical Resistivity
  • CTE, linear
  • Thermal Conductivity
  • Cadmium, Cd, <5 ppm by weight
  • Carbon, C, <100 ppm by weight
  • Iron, Fe, <30 ppm by weight
  • Lead, Pb, <5 ppm by weight
  • Mercury, Hg, <1 ppm by weight
  • Molybdenum, Mo
  • Oxygen, O
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Plansee SE

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.