MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
China-Yixing Longly Refractories Steatite Ceramics (High Frequency Porcelain)
Categories: Ceramic; Oxide; Magnesium Oxide; Silicon Oxide

Material Notes: LONGLY's steatite ceramics (namely high frequency porcelain, strengthened porcelain, magnesia porcelain), molecular formula as MgO-SiO2, is pure white. Steatite is the appropriate option when good mechanical properties and electrical resistance are needed, and is one of insulating materials with relatively good strength that operates safely at temperatures up to 1200°C. It has strong acid resistance, insulation property and absorbability, and is a kind of ceramic for mounting purposes, which can be used as coil skeleton, mounting panel, bracket, various high frequency insulator, band switch porcelain axis, porcelain bushing, seal housing, resistor cores and casings and so on in the electronic products. Steatite ceramics (high frequency porcelain) has high heat insulation performance, good chemical stability, high pressure resistance and stability of electric properties with temperature and frequency variation.

Information Provided by China Yixing Longly Refractories Co. Ltd

Vendors:
Available Properties
  • Density
  • Water Absorption
  • Hardness, Mohs
  • Flexural Strength, cold bending
  • Compressive Strength, Ambient
  • Volume Resistivity
  • Volume Resistivity
  • Dielectric Strength
  • Dielectric Strength, DC Breakdown Strength
  • Dielectric Strength, Insulating Strength
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Al2O3
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
China-Yixing Longly Refractories Co. Ltd

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.