MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Beryllium Copper, UNS C17200, TM05 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Mill-hardened Temper, TM - SHM

Fabrication Properties: Excellent Suitability – Capacity for Being Hot Formed; Good Suitability – Soldering, Brazing, Gas Shielded Arc Welding, Coated Metal Arc Welding, Spot Weld, Capacity for Being Cold Worked; Fair Suitability – Seam Weld, Butt Weld

Common Fabrication Processes: Blanking; Drawing; Drilling; Forming and Bending; Tapping; Turning

Typical uses: Belleville Washers; Clips; Connectors; Contact Bridges; Electrical Switch and Relay Blades; Fuse Clips; Navigational Instruments; Relay Parts; Spring Connectors, Current Carrying; Switch Parts; Bolts; Fasteners; Lock Washers; Retaining Rings; Roll Pins; Screws; Washers; Bearings; Bellows; Bourdon Tubes; Bushings; Diaphragms; Flexible Metal Hose; Housings for Instruments; Non Sparking Safety Tools; Pump Parts; Pumps; Rolling Mill Parts; Shafts; Spline Shafts; Springs; Springs, Electrochemical; Valve Seats; Valve Stems Valves; Wear Plates on Heavy Equipment; Welding Equipment; Firing Pins Tools

Applicable Specifications: Bar – AMS 4533, AMS 4534, AMS 4651, AMS 4650, ASTM B196/B196M, SAE J463, ASTM B194, MILITARY MIL-C-21657, SAE J461; Extrusions – ASTM B570; Forgings – AMS 4650, ASTM B570; Plate – AMS 4530, ASTM B194; Rod – AMS 4650, AMS 4533, MILITARY MIL-C-21657, SAE J463, SAE J461, ASTM B196/B196M, AMS 4534, AMS 4651; Shapes – AMS 4650; Sheet – ASTM B194, AMS 4530, AMS 4532; Strip – AMS 4532, ASTM B888/B88M, ASTM B194, SAE J463, SAE J461, AMS 4530; Tube – AMS 4535, ASTM B643; Wire – SAE J461, ASTM B197/B197M, SAE J463, AMS 4725

Vendors:
Available Properties
  • Density
  • Hardness, Rockwell C
  • Tensile Strength
  • Tensile Strength, Yield, 0.2% Offset
  • Elongation at Break
  • Tensile Modulus
  • Modulus of Rigidity
  • Poissons Ratio, Calculated
  • Machinability
  • Forgeability
  • Electrical Resistivity, 22% IACS
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Processing Temperature, Stress Relief
  • Solution Temperature, Water
  • Hot-Working Temperature
  • Precipitation Temperature, Air
  • Aluminum, Al
  • Beryllium, Be
  • Cobalt, Co
  • Copper, Cu, As Balance
  • Silicon, Si
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.