MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Arla MAKROCLEAR™ HARDCOAT PC Sheet
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Extruded

Material Notes: MAKROCLEAR™ HARDCOAT is a hard coated polycarbonate transparent sheet for flat applications. The high impact strength of polycarbonate is combined with a hard coating for flat applications, improved weatherability and chemical resistance and good protection against abrasion. MAKROCLEAR™ HARDCOAT has medium optical quality and is the choice when chemical resistance, scratch resistance and impact strength are more important than high optical clarity. MAKROCLEAR™ HARDCOAT is resistant to many of the most common chemicals, and the hard coat also provides an excellent protection against vandalism as paint and ink does not stick to the coated surface.

Benefits: Abrasion and Impact Resistant; UV Stability; Chemical resistance; More than 10 times the impact strength of high impact acrylic

Application: Anti-vandal glazing, security glazing, safety screens and acoustic screens, Industrial equipment (machine covers, machine protections), Indoor and outdoor signs, vending machine faces and many different kinds of technical parts.

Information provided by Arla Plast.

Vendors:
Available Properties
  • Density, ISO 1183
  • Moisture Absorption, ISO 62, 50% RH
  • Tensile Strength at Break, ISO 527
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527
  • Elongation at Yield, ISO 527
  • Modulus of Elasticity, ISO 527
  • Flexural Modulus, ISO 178
  • Izod Impact, Notched (ISO), ISO 180/1A
  • Izod Impact, Notched (ISO), ISO 180/1A
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact, Notched, ISO 179/1eA
  • Abrasion, ASTM D1044, % Haze; Taber, CS 10F, 500 cycles
  • CTE, linear, ISO 11359-2
  • Thermal Conductivity, DIN 8302
  • Refractive Index, ISO 489
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.