MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Master Bond EP41S-5Med Two component epoxy system
Categories: Polymer; Thermoset; Epoxy

Material Notes: Key Features:
  • Convenient handling
  • Easy to apply
  • Meets ISO 10993-5 specifications
  • Resists repeated autoclaving
Product Description: Master Bond EP41S-5Med is a two part epoxy system for bonding, sealing and coating, for use in medical devices. It has a forgiving 100 to 25 mix ratio by weight. It cures at room temperature or more rapidly at elevated temperatures, with the optimum being overnight at room temperature followed by 3-4 hours at 150-200°F. EP41S- 5Med has stellar resistance to a wide host of sterilants, including those derived from hydrogen peroxide. It also withstands acids, bases, and aggressive solvents. The system has no solvents or diluents, and low shrinkage upon curing. It bonds well to a wide variety of substrates including metals, composites, glass, ceramics, as well as many rubbers and plastics. This epoxy has very good physical strength properties and electrical insulation values. EP41S-5Med is serviceable over a wide temperature range of -80°F to +450°F. The standard color is black. This epoxy can be used for bonding and sealing in endoscopes, imaging systems, implantable devices, surgical instruments, sterilization chambers, as well as in medical electronics.

Product Advantages:

  • Easy to use
  • High glass transition temperature
  • Convenient packaging, available in a gun dispenser
  • Highly resistant to solvents, including ethanol
  • Withstands hydrogen peroxide based sterilants including Steris
  • Meets ISO 10993-5 specifications

Information provided by Master Bond.

Vendors:
Available Properties
  • Viscosity, Part B
  • Viscosity, Mixed
  • Viscosity, Part A
  • Hardness, Shore D
  • Tensile Strength
  • Adhesive Bond Strength, Tensile lap shear, Al to Al
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg
  • Cure Time, Option 2
  • Cure Time, Optimal: overnight at 75°F, plus 3-4 hours at 200°F
  • Cure Time, Option 1
  • Working Life, after mixing, 100 gram batch
  • Shelf Life, in syringes, in original, unopened containers
  • Shelf Life, in cans, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.