Available Properties |
---|
- Density, ISO 1183, DAM
- Linear Mold Shrinkage, Flow, ISO 294-4, 2577, DAM
- Linear Mold Shrinkage, Transverse, ISO 294-4, 2577, DAM
- Tensile Strength at Break, ISO 527-1/-2, 50% RH
- Tensile Strength at Break, ISO 527-1/-2, DAM
- Elongation at Break, ISO 527-1/-2, 50% RH
- Elongation at Break, ISO 527-1/-2, DAM
- Tensile Modulus, ISO 527-1/-2, DAM
- Tensile Modulus, ISO 527-1/-2, 50% RH
- Flexural Strength, ISO 178, 50% RH
- Flexural Strength, ISO 178, DAM
- Flexural Modulus, ISO 178, DAM
- Flexural Modulus, ISO 178, 50% RH
- Charpy Impact Unnotched, ISO 179/1eU, 50% RH
- Charpy Impact Unnotched, ISO 179/1eU, 50% RH
- Charpy Impact Unnotched, ISO 179/1eU, DAM
- Charpy Impact Unnotched, ISO 179/1eU, DAM
- Charpy Impact, Notched, ISO 179/1eA, 50% RH
- Charpy Impact, Notched, ISO 179/1eA, DAM
- Charpy Impact, Notched, ISO 179/1eA, DAM
- Volume Resistivity, IEC 62631-3-1, DAM
- Dielectric Strength, IEC 60243-1, DAM
- Comparative Tracking Index, IEC 60112, DAM
- CTE, linear, Parallel to Flow, ISO 11359-1/-2, DAM
- CTE, linear, Parallel to Flow, ISO 11359-1/-2, DAM
- CTE, linear, Parallel to Flow, ISO 11359-1/-2, DAM
- CTE, linear, Transverse to Flow, ISO 11359-1/-2, DAM
- CTE, linear, Transverse to Flow, ISO 11359-1/-2, DAM
- CTE, linear, Transverse to Flow, ISO 11359-1/-2, DAM
- Melting Point, ISO 11357-1/-3, first heat
- Melting Point, ISO 11357-1/-3, first heat
- Melting Point, ISO 11357-1/-3, first heat
- Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2, DAM
- UL RTI, Electrical, UL 746B, DAM
- UL RTI, Electrical, UL 746B, DAM
- UL RTI, Electrical, UL 746B
- UL RTI, Electrical, UL 746B
- UL RTI, Mechanical with Impact, UL 746B, DAM
- UL RTI, Mechanical with Impact, UL 746B
- UL RTI, Mechanical with Impact, UL 746B
- UL RTI, Mechanical with Impact, UL 746B
- UL RTI, Mechanical without Impact, UL 746B, DAM
- UL RTI, Mechanical without Impact, UL 746B
- UL RTI, Mechanical without Impact, UL 746B
- UL RTI, Mechanical without Impact, UL 746B
- Flammability, UL94, IEC 60695-11-10, DAM
- Flammability, UL94, IEC 60695-11-10, DAM
- Oxygen Index, ISO 4589-1/-2, DAM
- Glow Wire Ignition Temperature, IEC 60695-2-12, DAM
- Glow Wire Flammability Index, IEC 60695-2-12, DAM
- Melt Temperature, Injection
- Melt Temperature, Injection
- Melt Temperature, Injection
- Mold Temperature, Injection
- Mold Temperature, Injection
- Mold Temperature, Injection
- Drying Temperature, Injection
- Dry Time, Dehumidified Dryer; Injection
- Moisture Content, Injection
|
| | |