MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Goodfellow Tungsten Carbide/Cobalt
Categories: Ceramic; Carbide; Metal; Metal Matrix Composite

Material Notes: Tungsten Carbide is a hard, brittle ceramic which, when combined with 6% to 10% Cobalt, forms a tough Cermet (Ceramic-Metal). This material was developed for use in cutting tools, having hard ceramic crystals of a few microns in size within a ductile metal matrix. The resulting material can withstand the high compressive stresses imposed during cutting, as well as having good wear and oxidation resistance at the high temperatures reached. Tungsten Carbide/ Cobalt has a high resistance to thermal shock, so is able to withstand the rapid temperature fluctuations. Also, this has found a use as electrodes for Electrode Discharge Machining.

Information provided by Goodfellow.

Vendors:
Available Properties
  • Density
  • Vickers Microhardness, kg(f)/mm²
  • Tensile Strength at Break
  • Tensile Modulus
  • Compressive Strength
  • Electrical Resistivity
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Cobalt, Co
  • WC
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.