MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Go Yen Chemical GY-FROP54 Halogen-Free Synthetic Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: GY-FR-OP54 is a halogen-free synthetic flame retardant specially developed by GYC GROUP. It is not easily soluble in water or organic solvents. It has an excellent hydrolysis resistance, a good thermal stability, and a very high processing temperature range. It is recommended being used on fiber reinforced composites such as PBT, PA, POM, and other engineering plastics applications where high temperature manufacturing is required. GY-FR-OP54 provides an excellent fire-retardant performance and adds more value to your products.

Intro: Being the largest functional additives manufacturer in Taiwan, GYC Group has accumulated experience in the field of specialty chemicals for forty years. We not only offer total-solution services to the customers but constantly provide innovative and differentiated products to meet the customers’ requirements. GY-FR-OP54 is a halogen-free synthetic flame retardant specially developed by GYC GROUP. It is not easily soluble in water or organic solvents. It has an excellent hydrolysis resistance, a good thermal stability, and a very high processing temperature range. It is recommended being used on fiber reinforced composites such as PBT, PA, POM, and other engineering plastics applications where high temperature manufacturing is required. GY-FR-OP54 provides an excellent fire-retardant performance and adds more value to your products.

Advantages:

  • Excellent flame-retardant performance
  • Lasting flame-retardant effect
  • Excellent hydrolysis resistance
  • Good thermal stability
  • Can be processed under a high temperature
  • Good hydrolysis resistance
  • Environmental friendly (halogen free)
Applications:
  • PET
  • PBT
  • NYLON6, NYLON66
  • Various fiber-reinforced composite materials
  • Other plastic applications
  • Fireproof masterbatch

Information provided by Go Yen Chemical

Vendors:
Available Properties
  • Density
  • Decomposition Temperature
  • Moisture Content
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.