MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Syensqo (Solvay Specialty Polymers) Diofan® P 530 Polyvinylidene Chloride (PVDC)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyvinyl Dichloride (PVDC); Polyvinyl Dichloride (PVDC)

Material Notes: Diofan® P 530 is a one-component, water-based dispersion of a polyvinylidene chloride (PVDC) copolymer. It is free of solvent traces, alkylphenol ethoxylates or any other toxic substances. This material was developed to adhere on metal and to remain flexible when exposed to a broad range of end-use temperatures over time. This makes it an ideal binder for one-component, air drying, waterborne formulated paints and coatings where long-lasting protection of the substrate is targeted.

Diofan® P 530 also provides excellent chemical resistance and flame-retardant properties. Typical applications include Corrosion-resistant primers and coatings for industrial and heavy duty steel protection; Automotive primers and underbody coatings; Rust converter products; Barrier and sealing coatings; Flame-retardant coatings; Fibers and textile coatings

Chemical Resistant; Flame Retardant; Good Adhesion; Low VOC; Moisture Barrier; Non-Toxic; Oxygen Barrier

Uses: Coating Applications; Protective Coatings

Agency Ratings: EC 1907/2006 (REACH); EU No 10/2011

Availability: Asia Pacific; Europe; Latin America; North America

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Density
  • Density
  • pH
  • Glass Transition Temp, Tg, DSC
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.