Cerachem Fiber: Spun refractory fibers made, made from melted alumina, silica and zirconia. Typical applications: - Raw material for the manufacturing of finished products such as boards, paper, shapes, yarns etc.
- Loose insulating fill for complex space and areas where access is difficult
- Packing expansion joints
- Packing material for temporary repair of insulation
- Fiber reinforcement for insulating concretes and cements
- Precursor for engineered fibers
Information provided by Morgan Advanced Materials |