MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
BASF Ultramid® eXten D219WFC V50 BLACK Nylon 6.10, 50% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610); Nylon 610, Glass Reinforced

Material Notes: Product Description: Ultramid® eXten D 219WFC V50 black is a polyamide 6.10, reinforced with 50% of glass fiber, heat stabilized with organic stabilizers, for injection molding. This grade offers lower water uptake, higher dimensional stability and enhanced chlorine resistance versus standard PA 6.6. It offers too an enhanced corrosion resistance, a reduction in lead levels versus standard metal solutions and an increase in ease of processing and part design freedom versus metal solutions and other plastics. It is used for cold and warm water plumbing components including, but not limited to, components in contact with drinking water systems globally where elevated levels of chlorine could be present.

Availability: Asia Pacific; Europe; North America

Filler/Reinforcement: Glass Fiber, 50% Filler by Weight

Features: Chlorine Resistant; Corrosion Resistant; Good Dimensional Stability; Good Processability; Heat Stabilized – Organic; Low (to None) Lead Content; Low to No Water Absorption

Uses: Plumbing Parts; Potable Water Applications

Agency Ratings: ACS; DVGW W270; EC 1907/2006 (REACH); EU 2011/65/EC; EU 2015/863 RoHS3; KTW

Appearance: Black

Forms: Pellets

Processing Method: Injection Molding

Resin ID (ISO 1043): PA610-GF50

Information provided by BASF Corporation

Vendors:
Available Properties
  • Density, ISO 1183
  • Water Absorption, ISO 62
  • Water Absorption at Saturation, ISO 62
  • Maximum Moisture Content
  • Linear Mold Shrinkage, Flow, ISO 294-4
  • Linear Mold Shrinkage, Transverse, ISO 294-4
  • Tensile Strength at Break, ISO 527-2
  • Elongation at Break, ISO 527-2
  • Tensile Modulus, ISO 527-2
  • Flexural Strength, ASTM D790
  • Flexural Strength, ISO 178
  • Flexural Modulus, ASTM D790
  • Flexural Modulus, ISO 178
  • Izod Impact, Notched (ISO), ISO 180/A
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact, Notched, ISO 179/1eA
  • Volume Resistivity, IEC 62631-3-1
  • Dielectric Constant, IEC 62631-2-1
  • Dielectric Strength, IEC 60243-1
  • Comparative Tracking Index, IEC 60112, Solution A
  • Melting Point, ISO 11357-3
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-2/A, Unannealed
  • Flammability, UL94
  • Flammability, UL94
  • Glow Wire Flammability Index, IEC60695-2-12
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Mold Temperature
  • Drying Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.