MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Indorama Ventures Mexico Polyclear™ T-94 PET Resin
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Description: La resina Polyclear® PET T-94 de Arteva Specialities es un copolimero de baja velocidad de cristalizacion, ideal para la fabricacion de pared gruesa, con una viscosidad intrinseca de 0.86 dl/g. La resina Polyclear® PET T-94 tiene excelentes propiedades de cristalizacion y fundido, que facilita el proceso de inyeccion-estirado-soplado. La resina cumple con la regulación de la Federal Food, Drug and Cosmetic Act para aplicaciones especificas en alimentos. Para mayores detalles de la FDA, por favor contacte a Arteva Specialties. Los envases hechos con la resina Polyclear® PET T-94 son ligeros, irrompibles, tienen excelente brillo, transparencia y propiedades de barrera. Son atoxicos, se pueden pigmentar en una amplia gama de colores, y tienen la gran ventaja de ser totalmente reciclables.

Key Words: Exceptional clarity and color
Vendors:
Available Properties
  • Density, M2E-71-043, Limit
  • Density, M2E-71-043, Target
  • Apparent Bulk Density, M2E-72-015, Target
  • Apparent Bulk Density, M2E-72-015, Limit
  • Viscosity Measurement, M2E-75-011, Target
  • Viscosity Measurement, M2E-75-011, Limits
  • Crystallinity, M2E-71-043, Limit
  • Crystallinity, M2E-71-043, Target
  • Acetaldehyde, M2E-75-007, Target
  • Acetaldehyde, M2E-75-007, Limit
  • Melting Point, M2E-73-002, Target
  • Melting Point, M2E-73-002, Limits
  • Transmission, Visible, clear; thickness not quantified
  • Moisture Content, M2E-72-010, Target
  • Moisture Content, M2E-72-010, Limit
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.