Typical applications for Amodel® AS-1566 HS resin include electrical connectors and housings, motor components, pistons, covers, engine parts and transmission components.- Black: AS-1566 HS BK 324- Black: AS-1566 HS BK 545- Natural: AS-1566 HS NT
Key Attributes: Chemical Resistant; Creep Resistant; Good Dimensional Stability; Good Toughness; Heat Stabilized; High Heat Resistance; High Strength; Low CLTE; Ultra High Stiffness
Applications: Automotive Applications; Automotive Electronics; Automotive Under the Hood; General Purpose; Housings; Industrial Applications; Industrial Parts; Lawn and Garden Equipment; Machine/Mechanical Parts; Metal Replacement; Power/Other Tools; Thick-walled Parts; Valves/Valve Parts
Automotive Specifications: 3M 11-0003-5762-1 Color: NT Natural; ASTM D6779 PA122R65 Color: BK324 Black; ASTM D6779 PA122R65 Color: BK545 Black; ASTM D6779 PA122R65 Color: NT Natural; BMW GS 93016; DELPHI DCM4899 Color: BK324 Black; DELPHI DCM4899 Color: NT Natural; DELPHI M-2987 Color: BK324 Black; DELPHI M-2987 Color: NT Natural; DELPHI M-53292; DELPHI M-53292 Color: BK545 Black; GM GM7001M PA6T/6I/66 A3 A22 A42 A64 BJ721 DE1830 KS1750 Color: NT Natural; GM GMP.PPA.003 Color: Black; GM GMP.PPA.003 Color: Natural; GM GMW16358P-PPA-GF43MD22 Color: BK324 Black; GM GMW16358P-PPA-GF43MD22 Color: NT Natural; TRW SP-13161601 Color: BK324 Black
Injection Notes: Storage:- Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. Manufacturer recommendeds that Amodel® resins be dried prior to molding.
Data for dry samples unless noted.
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlastic