MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Zircar Refractory Composites SB-2000 SILICA BLANKET
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: ZIRCAR Silica Blanket Type SB-2000 is a high temperature insulation blanket made of mechanically interlocked continuous filament amorphous silica fibers with useful properties to temperatures of 1100°C (2012°F). SB-2000 is a strong needled blanket with very good handling properties. It is virtually shot free and has high resistance to attack by most chemicals. Exceptions include strong bases and hydrofluoric acid. This blanket exhibits thermal shock immunity, thermal conductivity and heat storage in the range of refractory ceramic fiber (RCF) blanket and is useful in many applications where RCF is not desired.

Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)

Vendors:
Available Properties
  • Density
  • Filament Diameter
  • Thermal Conductivity, ASTM C177, 1 in. blanket, 9.98 pcf (0.16 g/cc)
  • Thermal Conductivity, ASTM C177, 1 in. blanket, 9.98 pcf (0.16 g/cc)
  • Thermal Conductivity, ASTM C177, 1 in. blanket, 9.98 pcf (0.16 g/cc)
  • Thermal Conductivity, ASTM C177, 1 in. blanket, 9.98 pcf (0.16 g/cc)
  • Thermal Conductivity, ASTM C177, 1 in. blanket, 9.98 pcf (0.16 g/cc)
  • Melting Point
  • Maximum Service Temperature, Air
  • Shrinkage
  • Shrinkage
  • Shrinkage
  • Al2O3
  • B2O3
  • CaO
  • MgO
  • Other, Oxides
  • SiO2
  • TiO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Zircar Refractory Composites, Inc.

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.