Potential applications include automotive headlamp reflectors, fog lamp reflectors, park and turn reflectors, and other applications where excellent surface finish for direct metallization is desired.
Veradel® LTG-3301 resin is available in a variety of colors.- Veradel® LTG-3000 BK 184 MR (black)- Veradel® LTG-3301 NT MR (natural)- Veradel® A-301 BG 903 MR (beige)- Veradel® LTG-3000 GY 001 MR (gray)
Key Attributes: Creep Resistant; Good Dimensional Stability; Good Surface Finish; Good Thermal Stability; Good Toughness; High Flow; High Heat Resistance; Low Moisture Absorption
Applications: Automotive Applications; Automotive Exterior Trim; Metal Replacement; Reflectors