Features: Sealing applications with adhesion to PA. Applications: Grommets, Handles (Power tool) Fastenings, Cable clips, Seals, Flexible Connections, Membranes. MATERIAL ADVANTAGES: Insert molding possible, Adhesion to PA6 and PA6.6, up to 50% glass fiber, Optimized compression set, Colorable. Regulations / Approvals: UL 94 HB. General THERMOLAST® K information: Processing by multi-component injection molding with a wide range of thermoplastic materials such as PP, ABS, PC, PC/ABS, PBT, PETG, ASA, SAN, PMMA, PET, PA6/6.6/12, POM, PS, HIPS, etc. Excellent mechanical properties, High thermal stability, Excellent UV-, ozone, and weather resistance, Optimized for extrusion processes, also suitable for film extrusion, Free of latex, PVC, and phthalates, No use of heavy metals, Recyclable. Well established in the Automotive, Industry, and Consumer markets with various approvals. Information provided by Kraiburg TPE. A newer data sheet is available in MatWeb. |