MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Saint-Gobain Norton® V760 High Density Vibration
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Foam Grade

Material Notes: Description: Seals and Dampens Vibration: Norseal® V760 is a closed-cell PVC foam sealant with a pressure-sensitive adhesive on one side. Its high-density structure and multitude of tiny cells act like shock absorbers to seal and dampen vibration. Firm, High Density Foam for Positive Seals: This shock-absorbing feature makes Norseal V760 ideal for die-cut applications and metal-to-metal sealing. Versatile and easy to use, Norseal V760 is designed to produce a positive seal in mechanically fastened assemblies with as little as 30 percent compression. Conformable and Dimensionally Stable: Norseal V760 provides excellent conformability to curved and irregular shapes. It is resistant to weather, fungi and oxidation, ensuring a long sealing life. In addition, Norseal V760 is dimensionally stable. It will not drip, ooze or run under compression, and remains flexible at low temperatures. Pressure Sensitive Adhesive: The aggressive pressure-sensitive adhesive on one side of Norseal V760 facilitates high-speed application. The easy-peel paper liner eliminates stretching during installation, and removes easily after application. Norseal V760 series is available in gray. For specific low energy plastics, a specially formulated adhesive, "LE" is available.

FEATURES/BENEFITS:
  • Dimensionally stable under compression
  • Good abrasion resistance
  • Design facilitates high-speed application
  • Liner removes easily after application
  • Resistant to wether, fungi and oxidation
  • Low water absorption for long sealing life
  • Provides insulating properties
Applications: Truck trailer joint seals, door frame assemblies, concrete forms, export container seals, die-cut gaskets, roof sealing for parapets, duct seals, appliance seals, truck cab overlap seals. All data based on a 0.125 inch test sample.(Available in multiple thicknesses.)
Information provided by Saint Gobain Performance Products.

Vendors:
Available Properties
  • Density, ASTM D1667
  • Water Absorption, NTP-35, % by volume
  • Hardness, Shore OO, ASTM D2240
  • Tensile Strength, Yield, ASTM D-412 (Die A)
  • Elongation at Break, ASTM D-412 (Die A)
  • Compressive Strength, ASTM D1667, Compression Deflection, Compressed to 30%.
  • Compressive Modulus, ASTM D1667, Force to Compress, Value for 30% compression.
  • Compression Set, Norton Test Procedure 37, Constant Deflection, Compressed to 30%.
  • Thermal Conductivity, ASTM C-518
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saint Gobain Performance Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.