The sum of 'Other' metallic elements 0.010 percent or more each, expressed to the second decimal before determining the sum. The aluminum content for unalloyed aluminum not made by a refining process is the difference between 100.00 percent and the sum of all other metallic elements present in amounts of 0.010 percent or more each, expressed to the second decimal before determining the sum. Includes listed elements for which no specific limit is shown. This database entry lists the complete composition spec as collected by TheMetalMarket. Other database entries have complete physical property data for most aluminum alloys. |
UNS A03050 (Obsolete); Aluminium 305.0 |