MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Henkel Loctite® 3D IND405 3D Printing Resin, Black
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoset

Material Notes: Loctite® 3D IND405 is a rigid, high-strength, high elongation engineering material with outstanding impact resistance and excellent surface finish properties. This stiff and durable high-performance material is ideal for various tools on the production floor. Henkel Loctite® IND405 is a rigid polymer 3D printing resin designed for the DLP (Digital Light Processing) 3D printing process. IND405 has high elongation and toughness and is a one-part material with remarkable surface finish properties. These properties are comparable to an unfilled thermoplastic like polypropylene (PP).

Applications: manufacturing aids, tools, and housing. Fluid routing prototypes. Consumer goods.

Colors: black and clear

Vendors:
Available Properties
  • Specific Gravity
  • Density, ASTM D1475, Solid. Green.
  • Density, ASTM D1475, Solid. Post processed.
  • Volatiles, Liquid as Supplied
  • Viscosity, ASTM D7867, Liquid as Supplied
  • Hardness, Shore D
  • Hardness, Shore D
  • Hardness, Shore D, ASTM D648, Post processed.
  • Hardness, Shore D, ASTM D648, Post processed.
  • Tensile Strength at Break, ASTM D638, Green.
  • Tensile Strength at Break, ASTM D638, Post processed.
  • Tensile Strength at Break, ASTM D638, Post-processed
  • Tensile Strength at Break, ASTM D638, Post-processed
  • Tensile Strength at Break, ASTM D638, Post-processed
  • Tensile Strength, Yield, ASTM D638, Green.
  • Tensile Strength, Yield, ASTM D638, Post processed.
  • Tensile Strength, Yield, ASTM D638, Post-processed
  • Tensile Strength, Yield, ASTM D638, Post-processed
  • Elongation at Break, ASTM D638, Green.
  • Elongation at Break, ASTM D638, Post processed.
  • Elongation at Break, ASTM D638, Post-processed
  • Elongation at Break, ASTM D638, Post-processed
  • Elongation at Break, ASTM D638, Post-processed
  • Modulus of Elasticity
  • Modulus of Elasticity, ASTM D638, Post-processed
  • Modulus of Elasticity, ASTM D638, Post-processed
  • Modulus of Elasticity, ASTM D638, Post-processed
  • Tensile Modulus, ASTM D638, Post processed.
  • Tensile Modulus, ASTM D638, Green.
  • Izod Impact, Notched, ASTM D256
  • Volume Resistivity, ASTM D257
  • Surface Resistance, ASTM D257
  • Dielectric Constant, ASTM D150, AC, XY
  • Dielectric Constant, ASTM D150, AC, XY
  • Dielectric Constant, ASTM D150, AC, XY
  • Dielectric Strength, ASTM D149
  • Dissipation Factor, ASTM D150, AC, XY
  • Dissipation Factor, ASTM D150, AC, XY
  • Dissipation Factor, ASTM D150, AC, XY
  • CTE, linear, ASTM E831
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Flash Point, Liquid as Supplied
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.