MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Kohesi Bond KB 1458 TC Two component, unique epoxy offering extremely low thermal resistance
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive; Epoxy, Thermally Conductive

Material Notes: Product Highlights:
  • Excellent heat transfer efficiency
  • Low coefficient of thermal expansion (CTE)
  • Superb mechanical strength properties
  • Microns thin bond lines achievable
  • Phenomenal electrical insulation properties
  • Unlimited working life at room temperature
Kohesi Bond KB 1458 TC is a two component, thermal management epoxy system. This product offers high heat transfer capabilities. This product has very low thermal resistance and can be applied in layers as thin as 10 microns. The efficiency of heat transfer improves exceedingly with lower thermal resistance. This can be explained easily with the following formula: R = l/K [“R” is the thermal resistance; “l” is the adhesive layer thickness; “K” is the thermal conductivity of the adhesive] Applying peculiar values, standard thermally conductive adhesives (alumina filled) that are applicable in more than 50 micron thicknesses, offer a thermal resistance of 35 - 40 × 10-6 m2•K/W. Since KB 1458 TC can be applied in 10 micron thick sections, it offers a notably low thermal resistance of 5 - 6 × 10-6 m2•K/W. KB 1458 TC has a wide service temperature range of -70°C to +150°C. It adheres well to a wide variety of substrates including metals, ceramics, composites, most plastics and glass. It provides superior bonding and physical strength properties and very low shrinkage upon cure. It offers excellent dimensional stability and a very low coefficient of thermal expansion (CTE). Part A and Part B are gray in color. Owing to its sensational thermal management properties KB 1458 TC is widely used in electronics, optical and specialty OEM industries.

Typical Applications:

  • Bonding
  • Sealing

Information provided by Kohesi Bond Custom Engineered Adhesives

Vendors:
Available Properties
  • Viscosity, Part B
  • Tensile Strength
  • Tensile Modulus
  • Adhesive Bond Strength, Tensile Lap Shear, Al/Al
  • Volume Resistivity
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time, Optimum Cure: Overnight at 23°C, followed by 3-5 hours at 90°C
  • Cure Time, Option 2
  • Cure Time, Option 1
  • Working Life, 100 g of mixed epoxy
  • Shelf Life, in original unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.