  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Chemours Teflon™ PFA 416HP Special purpose fluoroplastic resin
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA); Polyperfluoroalkoxyethylene, Molded/Extruded

Material Notes: Teflon™ PFA 416HP is a special purpose fluoroplastic resin available in pellet form. This resin has a higher melt flow rate (typical MFR of 42) than most other PFA fluoroplastic resins, which permits higher extrusion speed and easier processing, making Teflon™ PFA 416HP a cost effective alternative for producing thin-wall and complicated articles. Applications for Teflon™ PFA 416HP include high performance thin wall wire coatings; intricate injection molded parts for production of chemicals where purity in the parts-per-billion range is needed; semiconductor components and electronic parts; and fluid handling systems for high performance chemical filters. With a typical melt flow rate (MFR) of 42, Teflon™ PFA 416HP resin is ideally suited for applications requiring a high processing speed and very low viscosity.

Information provided by Chemours.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Water Absorption, ASTM D570
  • Melt Flow, ASTM D3307
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength, ASTM D3307
  • Elongation, Ultimate, ASTM D3307
  • Flexural Modulus, ASTM D790
  • Flex Crack Resistance, ASTM D2176, Cycles MIT Folding Endurance
  • Volume Resistivity, ASTM D257
  • Surface Resistivity per Square, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149, Short Time
  • Dissipation Factor, ASTM D150
  • Arc Resistance, ASTM D495
  • Melting Point, ASTM D4591
  • Maximum Service Temperature, Air, Continuous, per accelerated heat-aging test
  • Flammability, UL94
  • Oxygen Index, ASTM D2863
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Chemours, former DuPont

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.