Aquivion® D79-25BS is a chemically-stabilized (denoted by S-suffix) perfluorosulfonic acid (PFSA) ionomer dispersion that exhibits an Equivalent Weight (EW) of 790 g/eq. Polymer concentration is 25%. Solvent system is >99% water and is free of ethers. Aquivion® PFSA dispersions are based on the Short Side Chain copolymer of Tetrafluoroethylene (TFE) and Sulfonyl Fluoride Vinyl Ether (SFVE) F2C=CF-O-CF2CF2-SO2F produced by Solvay. The PFSA ionomer dispersions contain its acid form (-SO3H) and are available in various solvent systems, EWs and concentrations. These dispersions can be used to produce PEM fuel cell electrodes and electrochemical cell electrodes, to manufacture or repair ion exchange membranes, to produce super-acid catalysts, and for the surface treatment of PTFE membranes to improve wetting behavior. HEALTH, SAFETY AND ENVIRONMENT - Aquivion® PFSA dispersions are not harmful if used and handled according to standard processing procedures (see for example the "Guide to the Safe Handling of Fluoropolymer Resins" issued by the Society of the Plastics Industry). If handled inappropriately (e.g. overheating above 260°C (500°F) for extended period of time) the dispersions may release harmful toxic chemicals. By their chemical properties Aquivion® PFSA dispersion grades are classified as hazardous material subject to transportation regulations (ADR, IATA, IMDG). Specifically D79-25BS is corrosive (R-SO3H being a strong acid, measured pH < 2). Please refer to corresponding Material Safety Data Sheets for more information on handling and safety. PACKAGING, SHIPMENT AND STORAGE - Aquivion® PFSA D79-25BS is available in 0.25, 0.5 and 60 liter containers. It is recommended to store the product at 25°C (77°F) in a clean temperature-controlled and well ventilated environment, protected from direct sunlight and other sources of heat or irradiation. Containers should be kept tightly closed to avoid solvent evaporation. Information provided by Solvay Specialty Polymers. |