TECNOFLON® P 959 is a medium viscosity, high fluorine (70%), peroxide curable fluoroelastomer. Tecnoflon® P 959 exhibits superior resistance to a wide variety of chemicals, coupled with excellent processability and optimum compression set. Tecnoflon® P 959 can be cross-linked using organic peroxides in conjunction with a co-agent. Alcohol Resistant; Chemical Resistant; Crosslinkable; Fuel Resistant; Good Flow; Good Mold Release; Good Processability; Low Compression Set; Medium Viscosity; Steam Resistant Uses: Belts/Belt Repair; Blending; Gaskets; Hose; Profiles; Seals; Sheet; Valves/Valve Parts Processing: Calendering; Compounding; Compression Molding; Extrusion; Injection Molding; Resin Transfer Molding Availability: Europe; North America Information provided by Solvay Specialty Polymers. |