MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Polyplastics TOPAS® 8007F-600 COC  (Unverified Data**)
Categories: Polymer; Film; Thermoplastic; Cyclo Olefin Polymer

Material Notes: A standard extrusion grade with improved processability versus grade 8007F-04. Glass transition temperature (Tg) and viscosity are on a par with grade 8007F-04, while as is the case with grade 9506F-500, clarity is inferior and the haze value becomes high in films depending on the extrusion parameters. Use is recommended with high compression ratio olefin screws and in blends with PE.

TOPAS is an amorphous copolymer based on the polymerization of ethylene and nor-bornene using metallocene catalysts. Its property profile can be varied over a wide range by adjusting the chemical structure during polymerization.

Information provided by Polyplastics.

Vendors:
Available Properties
  • Density, ISO 1183
  • Water Absorption at Saturation, ISO 62
  • Moisture Vapor Transmission, ISO 15106-3, 90% RH
  • Melt Flow, ISO 1133
  • Melt Flow, ISO 1133
  • Film Elongation at Break, MD, ISO 527-3
  • Film Elongation at Break, TD, ISO 527-3
  • Tensile Modulus, ISO 527-3, Film, TD
  • Tensile Modulus, ISO 527-3, Film, MD
  • Film Tensile Strength at Break, MD, ISO 527-3
  • Film Tensile Strength at Break, TD, ISO 527-3
  • Glass Transition Temp, Tg, ISO 11357-1,-2,-3, 10°C/min
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Polyplastics Co.

Category Notes
Plastic

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.