MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
SABIC NORYL™ GFN2 PPE+PS (Americas)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polystyrene (PS)

Material Notes: NORYL™ GFN2 resin is a 20% glass reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This general-purpose injection moldable grade exhibits very low moisture absorption, high strength, hydrolytic stability, Low warpage, low specific gravity, and dimensional stability. NORYL GFN2 carries a UL746C outdoor suitability rating of F1 and is an excellent candidate for a variety of indoor and outdoor applications including construction, electrical components + displays, lawn and garden equipment. *See NORYL GFN2F resin for FDA food compliant / NSF version.

Information provided by SABIC

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Water Absorption, ASTM D570, 24hrs
  • Loss On Ignition, ASTM D2863
  • Linear Mold Shrinkage, Flow, SABIC method
  • Melt Flow, ISO 1133, MVR [cc/10 min]
  • Melt Flow, ASTM D1238
  • Hardness, Rockwell L, ASTM D785
  • Tensile Strength at Break, ASTM D638, 5 mm/min
  • Tensile Strength at Break, ISO 527, 5 mm/min
  • Elongation at Break, ISO 527, 5 mm/min
  • Elongation at Break, ASTM D638, 5 mm/min
  • Tensile Modulus, ASTM D638, 5 mm/min
  • Tensile Modulus, ISO 527, 1 mm/min
  • Flexural Yield Strength, ASTM D790, 1.3 mm/min, 50 mm span
  • Flexural Yield Strength, ISO 178, 2 mm/min
  • Flexural Modulus, ASTM D790, 1.3 mm/min, 50 mm span
  • Flexural Modulus, ISO 178, 2 mm/min
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D4812
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*4
  • Charpy Impact, Notched, ISO 179/2C
  • Instrumented Impact Total Energy, ASTM D3763
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149, in oil
  • Dissipation Factor, ASTM D150
  • Arc Resistance, ASTM D495
  • Hot Wire Ignition, HWI, UL 746A
  • Hot Wire Ignition, HWI, UL 746A
  • High Amp Arc Ignition, HAI, UL 746A
  • High Amp Arc Ignition, HAI, UL 746A
  • High Voltage Arc-Tracking Rate, HVTR, UL 746A
  • CTE, linear, Parallel to Flow, ASTM E831
  • CTE, linear, Transverse to Flow, ASTM E831
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75/Be, Edgew 120*10*4 sp=100mm
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, unannealed
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75/Ae, Edgew 120*10*4 sp=100mm
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, unannealed
  • Vicat Softening Point, ISO 306, Rate B/50
  • Vicat Softening Point, ISO 306, Rate B/120
  • UL RTI, Electrical, UL 746B
  • UL RTI, Mechanical with Impact, UL 746B
  • UL RTI, Mechanical without Impact, UL 746B
  • Flammability, UL94, UL 94
  • Nozzle Temperature, Injection Molding
  • Zone 1
  • Zone 2, Injection Molding
  • Zone 3
  • Melt Temperature, Injection Molding
  • Mold Temperature
  • Drying Temperature, Injection Molding
  • Dry Time, Injection Molding
  • Dry Time, Cumulative; Injection Molding
  • Moisture Content, Injection Molding
  • Back Pressure
  • Shot Size
  • Screw Speed
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saudi Basic Industries Corporation; SABIC Innovative Plastics (GE Plastics)

Category Notes
Plastic

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.