MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Morgan Advanced Ceramics Blakite Ceramic  (Unverified Data**)
Categories: Ceramic; Oxide

Material Notes: Super Duty. Morgan Thermal Ceramics refractory mortars are normally supplied as ready-to-use wet blends of finely-ground aggregates and special binders. They develop good strength on air drying, forming strong joints and conferring an almost monolithic structure to the brickwork. This is a highly refractory mortar, dark grey in colour, which has a high water retention characteristic. It was specially developed for laying insulating firebricks but is also suitable for use with super duty and high alumina dense refractory bricks, at operating temperatures up to 1650°C. It is supplied in a consistency uitable for shallow patching or trowelling but requires the addition of approximately 5% water for dipping. Blakite is a good choice as a single, general purpose mortar on projects involving mainly insulating firebricks but also including some dense firebricks

Applications:

  • For laying insulating firebricks, super-duty and high alumina dense refractory bricks
  • Provide resistance to infiltration of air or hot gases
  • Hobby and laboratory kilns
  • Retard penetration of slag and molten metal into the joints

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors:
Available Properties
  • Density, as applied
  • Linear Mold Shrinkage, dried
  • Modulus of Rupture
  • Maximum Service Temperature, Air, normal oxidizing conditions
  • Al2O3
  • CaO+MgO
  • Fe2O3
  • K2O+Na2O
  • SiO2
  • TiO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.