MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Arla ATECH® 3200 ABS Sheet
Categories: Polymer; Thermoset; Phenolic

Material Notes: ATECH is a series of sheets based on ABS which is a raw material with very high impact-strength. ABS also has impressive thermal qualities and is easy to thermoform and fabricate. The ATECH 3200 is a super high impact ABS with a top layer of high gloss PMMA (acrylic).
Also Available In: ATECH 3203 with extra UV stabilization added in ABS to improve weather resistance (3-5y); ATECH 3206 with extra UV stabilization added in ABS and PMMA (10y); Optional with different structures to combine the high gloss surface; Dual coloring to optimize to specific needs
Recycling: The total recycling concept (TRC) covers all types of sheets to provide cost savings. Off-cuts from the sheets can be used in production of new sheets by co-extruding virgin material as the top layer. Care is taken that all quality requirements are met.

Benefits: Super high gloss surface finish; Different stages of weathering performance solutions; Easy to thermoform; High impact strength; Good thermal qualities

Application: Suitable for demanding external automotive component parts which are exposed to UV light, and other tough industrial applications where a high gloss finish is required.

Information provided by Arla Plast.

Vendors:
Available Properties
  • Density, ISO 1183
  • Linear Mold Shrinkage, ISO 294-4
  • Ball Indentation Hardness, ISO 2039
  • Tensile Strength at Break, ISO 527-2
  • Tensile Strength, ISO 527-2
  • Tensile Strength, Yield, ISO 527-2
  • Elongation at Break, ISO 527-2, at Tensile strength
  • Elongation at Break, ISO 527-2
  • Elongation at Yield, ISO 527-2
  • Tensile Modulus, ISO 527-2
  • Flexural Strength, ISO 178
  • Flexural Modulus, ISO 178
  • Izod Impact, Notched (ISO), ISO 180/A
  • Izod Impact, Notched (ISO), ISO 180/A
  • Izod Impact, Notched (ISO), ISO 180/A
  • Charpy Impact, Notched, ISO 180/A
  • Charpy Impact, Notched, ISO 180/A
  • Charpy Impact, Notched, ISO 180/A
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-2
  • Vicat Softening Point, ISO 306, B120
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.