MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Lord Adhesives Thermoset™ UR-325 Urethane Encapsulant System
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: LORD Thermoset UR-325 encapsulant is a two-component urethane system designed for encapsulating delicate, pressure or shock sensitive electronic components. Thermoset UR-325 encapsulant cures to a low modulus material using room temperature cure. If stored or shipped at cooler temperatures, Thermoset UR-325 hardener may crystallize. If crystals appear, gently warm hardener at 32-46°C and periodically stir as it is liquefying. Heating period should not exceed three hours as excessive heating will cause dimerization.

Features: provides good adhesion to a variety of materials. can be used on parts and devices that experience operating temperatures from -90°C to +130°C. provides excellent thermal shock resistance; exhibits exceptional hydrolytic stability.

All information provided by Lord.

Vendors:
Available Properties
  • Specific Gravity, Mixed
  • Viscosity, Mixed
  • Hardness, Shore A, ASTM D 2240
  • Tensile Strength, ASTM D638, cured
  • Elongation at Break, ASTM D 638
  • Volume Resistivity, ASTM D 257, cured
  • Dielectric Constant, ASTM D 150, cured
  • Dielectric Strength, cured
  • Dissipation Factor, ASTM D 150, cured
  • CTE, linear, ASTM D 3386, cured
  • Thermal Conductivity, cured
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg, cured
  • Working Life, Mixed
  • Shelf Life, UR-325 Resin
  • Shelf Life, UR-325 Hardener
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.