MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Ravago Manufacturing Americas Ravatuf™ X45D FR Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Product Description: RAVATUF X45D FR is a semi-rigid Flame Retardant Thermoplastic Olefin (TPO) designed for applications requiring a balance of impact resistance, good scratch and mar, and dimensional stability over a broad temperature range. RAVATUF X45D FR can be used for both extrusion and molding applications. This product meets the UL 94 V0 flame rating.
Features: Molding grade with good dimensional stability and low shrinkage of 1.0% on average; Ease of coloring by using PE or PP based color concentrates; Ease of processing; Recyclability

Availability: North America

Features: Flame Retardant; Good Colorability; Good Dimensional Stability; Good Impact Resistance; Good Processability; Good Scratch Resistance; Low Shrinkage; Recyclable Material; Semi Rigid

Processing Method: Extrusion; Injection Molding

Information provided by Ravago Manufacturing Americas

Vendors:
Available Properties
  • Density, ASTM D792
  • Melt Flow, ASTM D1238
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Break, ASTM D638
  • Flexural Modulus, ASTM D790, 1% Tangent, 0.05 min/min
  • Izod Impact, Notched, ASTM D256
  • Gardner Impact, ASTM D5420
  • Tear Strength, ASTM D624
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, Unannealed
  • Brittleness Temperature, ASTM D746
  • Flammability, UL94
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Nozzle Temperature
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  • Screw Speed
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.